The building sector is a significant contributor to global energy consumption, necessitating the development of innovative materials to improve energy efficiency and sustainability. Phase change material (PCM)-enhanced concrete offers a promising solution by enhancing thermal energy storage (TES) and reducing energy demands for heating and cooling in buildings. However, challenges related to PCM leakage, mechanical strength reduction, and encapsulation durability hinder widespread adoption. This paper critically reviews the various PCM incorporation techniques and evaluates their impact on thermal performance and structural integrity. Our findings revealed that while PCM integration improves thermal efficiency, it reduces mechanical strength, especially at higher PCM content. To address these challenges, recent work emphasizes advancements in encapsulation technologies and thermal property optimization, focusing on mitigating leakage and enhancing durability. Organic PCM types are favored for concrete applications due to their compatibility, though issues with leakage control and strength retention remain unresolved. Hence, the choice of incorporation technique must balance application requirements, allowable mechanical property reductions, and cost constraints. Moreover, the lack of standardized methods to assess long-term PCM-composite durability highlights a need for further development of PCM encapsulation and integration techniques to optimize thermal and structural performance.
Reinforced concrete durability depends on a passive oxide film protecting embedded steel, sustained by high-alkalinity pore solutions. Cracking fundamentally alters transport, allowing rapid chloride and carbon dioxide ingress, which undermines passivity and accelerates corrosion. Self-healing concrete technologies aim to autonomously restore transport barriers and reestablish electrochemical stability. This review critically synthesizes evidence on healing effectiveness for corrosion mitigation through a dual framework of barrier restoration and interface stabilization, integrating depth-resolved chloride profiles with electrochemical performance indices. Critically, visual crack closure proves an unreliable indicator of corrosion protection. Healing mechanisms exhibit characteristic spatial signatures: autogenous and microbial approaches preferentially seal surface zones with diminishing effectiveness at reinforcement depth, while encapsulated low-viscosity polymers achieve greater depth continuity. However, electrochemical recovery consistently lags transport recovery, with healed specimens achieving only partial restoration of intact corrosion resistance. Recovery effectiveness depends on crack geometry, moisture conditions, and healing mechanism characteristics, with systems performing effectively only within narrow, condition-specific windows. Effective corrosion protection requires coordinated barrier and interface strategies targeting both bulk transport and steel surface chemistry. The path forward demands rigorous field validation emphasizing electrochemical outcomes over appearance metrics, long-term durability assessment, and performance-based verification frameworks to enable predictable service life extension.
7 April 2026 in Transportation Research Record: Journal of the Transportation Research Board
Ultra-high-performance concrete (UHPC) is increasingly used in modern infrastructure because of its outstanding strength and durability, but accurately measuring its tensile behavior remains a significant challenge. Direct-tension testing using AASHTO T 397, particularly with a 220 kip wedge grip machine, has been documented to yield success rates as low as 36%. This paper addresses direct-tension testing challenges by evaluating non-proprietary UHPC mixtures with steel fiber dosages from 0.0% to 2.0% and silica fume contents of 9%, 12%, and 15% of total binder content, all tested at 28 days. Through a two-phase experimental program, this study covers improvements to specimen preparation, machine alignment, and grip pressure. These refinements increased the test success rate to 75% with the same testing equipment. The results show that the amount of fiber is the primary factor influencing tensile strength and post-cracking performance of UHPC, while moderate changes in silica fume content have only a minor effect. This study provides a practical and repeatable test protocol for direct-tension evaluation and demonstrates that optimizing fiber dosage is essential to achieve the desirable tensile behavior of UHPC. The proposed approach enables confident material selection and promotes wider use of UHPC.