The use of vibratory welding is treated with some caution in the industry due to inconsistent beneficiary results. Here, a partial explanation is suggested by the differentiation between global vibrational effects (GVEs) and local vibrational effects (LVEs), and the latter is investigated experimentally. Two structural plates of steel are welded at three frequency/amplitude combinations using manual gas metal arc welding in an experimental setup that ensures only LVEs. After welding, tensile tests, microhardness tests, and metallurgical characterization are performed locally in the different welding zones and the results are compared to the non-vibrated welds. Novel use of digital image correlation (DIC) is implemented in tensile testing of welded samples, thus enabling the separate determination of local mechanical properties of the base metal, heat-affected zone and fusion zone of the same weld. LVE is found not to promote any distinct difference in weld properties, at least within the vibrational regimes studied. Nevertheless, depending on geometry and structural response, it is explained how vibratory welding may promote residual stress relief due to GVEs of the welded structure.
Additive manufacturing (AM) refers to advanced technologies for building 3D objects by adding material layer upon layer using either electron beam melting (EBM) or selective laser melting. AM allows us to produce lighter and more complex parts. However, various defects are created during the AM process, which severely affect fatigue behavior. In the current research, the effects of the anisotropic microstructure in the in-plane and out-of-plane orientations and defects on the fatigue crack propagation rate (FCPR) and crack path were studied. A resonance machine was used to determine the fatigue crack propagation rate (da/dN vs. ΔK) from the near-threshold up to the final fracture, accompanied by in situ Acoustic Emission (AE) monitoring. Micro-Computerized Tomography (µCT) enabled us to characterize surface and microstructural defects. Metallography was used to determine the microstructure vs. orientations and fractography to classify the fatigue fracture propagation modes. Calculations of the local stress distribution were performed to determine the interactions of the cracks with the defects. In the out-of-plane direction, the material exhibited high fatigue fracture toughness accompanied by a slightly lower fatigue crack propagation rate as compared to in-plane orientations. The near-threshold stress intensity factor was slightly higher in the out-of-plane orientation as compared to that in the in-plane one, accompanied by a lower exponent of the Paris law regime. The threshold decreased with an increasing load ratio as expected for both orientations. The crack propagation direction that crosses the elongated grains plays an important role in increasing fatigue resistance in the out-of-plane direction. In the in-plane directions, the crack propagates parallel to the grain boundary, interacts with more defects and exhibits more brittle striations on the fracture surface, resulting in lower fatigue resistance.
Women with silicone-gel breast implants may be at risk of burns on reconstructed tissue due to inadequate blood flow and heat transfer after mastectomy. This study employed thermal imaging and numerical simulations to examine the impact of external heat on silicone breast implants. By applying infrared radiation across three spectrum ranges, detailed thermal maps were created and analyzed with MATLAB software (Mathworks, Natick, MA, USA) version release 2020b. Implants were heated to simulate body and external conditions, enabling thermal imaging to assess temperature distribution. The Finite Element Method was utilized for heat transfer simulations. Our results indicated deeper thermal penetration in the implanted breast model compared to a standard model. This study highlights thermal imaging as a reliable, non-invasive method to evaluate implant responses to heat and suggests strategies to reduce heat-related injuries in patients with breast reconstruction. This method has the potential for comfortable and safe home monitoring of patients using handheld thermal imaging cameras that are now available as attachments for smartphones.
Metal additive manufacturing enables the production of complex Ti-6Al-4V components, but internal defects may form during processing and remain difficult to detect by visual inspection. This paper presents an automated acoustic tap-testing system for repeatable non-destructive evaluation of additively manufactured Ti-6Al-4V specimens. The system combines controlled mechanical excitation, longitudinal positioning, specimen rotation and elevation, soft mechanical isolation, and contact-free acoustic measurement to acquire consistent resonance-based responses. Candidate support materials were evaluated to approximate free-free boundary conditions, and finite-element modal simulations were used to relate measured spectral peaks to elastic vibration modes and support system calibration. Experimental verification showed dominant resonance bands around 4 kHz and 12.5 kHz, consistent with the adjusted modal simulation. A repeatability test on 40 specimens showed stable acoustic energy levels of approximately 109–115 dB, with no signal saturation. These results demonstrate that the developed platform reduces operator dependence, enables repeatable acoustic data acquisition, and provides a controlled basis for future classification of internal defects in additively manufactured metal components.
Ultra-high-performance fiber-reinforced concrete (UHPFRC) combines high strength and ductility, yet the influence of loading history on its fracture process zone (FPZ) and damage localization remains insufficiently understood. This study investigates flexural damage evolution in UHPFRC under three-point bending using an integrated acoustic emission (AE) and X-ray micro-computed tomography (μCT) framework. First, a UHPFRC prism is subjected to increasing cyclic peak loads of 6, 8, and 14 kN, with AE monitoring during loading and μCT scans after each peak to resolve progressive internal damage and crack morphology. The AE indices (hit rate, cumulative energy, b-value, and RA–AF classification) show a transition from matrix-dominated micro cracking at low loads to a history-dependent, highly localized FPZ governed by a few long rise time, high energy, fiber dominated events at the highest load, corroborated by μCT slices evolving from faint distributed cracks to a coalesced macrocrack with secondary branches and active fiber bridging. A nominally identical prism is then tested monotonically to fracture to establish a four-stage reference response: a fully elastic regime, a micro cracking regime at the first-cracking load (FCL), a macro cracking regime initiated at the bend-over point (BOP), and a post-peak softening regime in which the fibers act as bridges and delay final failure. Under monotonic loading, AE and μCT jointly indicate an extended, fiber-bridged FPZ with markedly higher shear-mode activity (≈ 21 % vs. 11–13 % across cyclic stages) and substantially greater total AE energy than under cyclic loading. The shear-mode enhancement is concentrated in the post-peak softening regime, where pure fiber pull-out and frictional sliding dominate. The combined AE and μCT framework provides calibrated AE thresholds for distinguishing service-level micro cracking from critical macrocrack localization in UHPFRC under cyclic bending, supporting performance-based design and structural health monitoring of fatigue-sensitive members.