In order to evaluate the effect and mechanism of composite modifiers on the anti-aging property of asphalt, this study selected hydrotalcite and ultraviolet absorber as anti-aging modifiers to prepare different types of modified asphalt and carry out ultraviolet aging treatment. The effects of composite modification on the physical and rheological properties of asphalt under ultraviolet aging conditions were studied by three indices and by dynamic shear rheometer. The distribution and interaction characteristics of composite modifiers in asphalt matrix were analyzed by scanning electron microscopy (SEM) and energy dispersion spectroscopy (EDS). Fourier transform infrared spectroscopy (FTIR) was used to analyze the changes in functional groups and characteristic parameters in the compound modified asphalt. Based on this, a molecular dynamics model of the compound modified asphalt was constructed, and the changes in solubility parameters, free volume, and mean azimuth shift were analyzed. The results show that the addition of the compound modifier can significantly improve the UV aging resistance of asphalt, mainly by controlling the asphalt components and characteristic functional groups, and the good compatibility between the modifier and asphalt ensures the modification effect.
The objective of this study is to systematically evaluate the reinforcement mechanisms of layered double hydroxides (LDHs) on the aggregate–asphalt interfacial adhesion in granite–asphalt systems under accelerated ultraviolet (UV) aging. The interfacial bonding durability of granite–asphalt composite systems is persistently threatened by hydrothermal stripping and UV weathering. A multiscale experimental framework comprising boiling kinetic tests, photoelectric colorimetry, and surface free energy (SFE) analysis based on the van Oss–Chaudhury–Good theory was executed, complemented by cross-sectional scanning electron microscopy (SEM). Macroscopic results demonstrate that a 3.0 wt.% LDH threshold optimizes the hydrothermal adhesion rating to Level 5. Thermodynamically, introducing 4.5 wt.% LDHs triggers a 176.37% surge in the polar SFE component (), causing the dry adhesion work () to peak and the wet stripping work () to plummet by 45.03%, verifying a significantly compressed driving force for moisture displacement. A reconciliation of these dosage-dependent results establishes 4.5 wt.% as the scientifically optimal formulation for maximizing long-term thermodynamic stability. Microstructural SEM analysis reveals that LDHs transition the terminal UV-degradation behavior from severe, reticulated brittle macro-cracking into highly controlled, damage-tolerant micro-fissuring. These findings provide thermodynamic targets and mechanistic insights that can guide the design of durable, weather-resistant asphalt pavements.