Two types of carbon nanotubes [single walled nanotubes (SWCNTs) and multi walled carbon nanotubes (MWCNTs)] are deposited on porous silicon by the drop casting technique. Upon exposure to test gas mixing ratio 3% NO2, the sensitivity response results show that the SWCNTs’ sensitivity reaches to 79.8%, where MWCNTs’ is 59.6%. The study shows that sensitivity response of the films increases with an increase in the operating temperature up to 200° and 150° for MWCNTs and SWCNTs. The response and recovery time is about 19 s and 54 s at 200° for MWCNTs, respectively, and 20 s and 56 s at 150° for SWCNTs.
9 October 2018 in Materials for Renewable and Sustainable Energy
CdS nanoparticles have been prepared by a chemical method and deposited as a thin film on both P-type silicon and porous silicon (PS) substrates by spin coating technique as a photoconductive detector. The Hall measurements show that the nanoparticles are n-type with carrier concentration of about (− 5.45 × 1010 cm−3). The response time of the fabricated detectors on Si, PS and (CdS + TPD/PS) substrates was measured (by illuminating the sample with Halogen lamp 250 W) and its values are 5.2 ms, 2.1 ms and 1.3 ms, respectively. The specific detectivity and photoresponsivity of the fabricated detector on PS are found to be (9.9 × 1012 Watt−1 Hz1/2 cm−1 and 0.043 A/W). The surface functionalization of the CdS nanoparticles film deposited on porous silicon (PS) substrate by triphenyldiamine (TPD) has highly improved the photoresponsivity and response time of the detector to 0.059 A/W and 1.3 ms.
12 December 2018 in IOP Conference Series: Materials Science and Engineering
Pure single walled carbon nanotubes (pure-SWCNTs) and Functionalized single walled nanotubes (F-SSWCNTs) have been utilized to the manufactured nitrogen dioxide gas sensor. CNTs films have been deposited on (n-type) silicon and porous silicon substrate by drop casting method. A porous silicon layer (PS) was prepared via electrochemical etching. The applied current density was 20 mA / cm2, and the typical electrochemical-etching time was chosen to be about 20 minutes. Upon exposure to fixed test gas mixing ratio (air: gas) NO2 at different operating temperatures, the sensitivity response results show that Pure single walled carbon nanotubes and Functionalized single walled nanotubes deposited on porous silicon have better performances than that deposited on silicon. At RT the F-SWCNTs/Ps sensitivity reaches to 36%, the response and recovery time is about 11 s and 26 s, whereas for SWCNTs/Ps the sensitivity 13.5%, the response and recovery time is about 13 s and 24 s.
1 January 2019 in Journal of Nano- and Electronic Physics
Journal of Nano- and Electronic Physics. Scientific journal. ISSN: 2077-6772. Journal abbreviation: J. Nano- Electron. Phys. No page charges. All articles are freely available on-line. Issued 4 times per year. Publisher: Sumy State University. (Sumy, Ukraine)