Controllable synthesis of homochiral nano/micromaterials has been a constant challenge for fabricating various stimuli-responsive chiral sensors. To provide an avenue to this goal, we report electrospinning as a simple and economical strategy to form continuous homochiral microfibers with strain-sensitive chiroptical properties. First, electrospun homochiral microfibers from self-assembled cadmium sulfide (CdS) quantum dot magic-sized clusters (MSCs) are produced. Highly sensitive and reversible strain sensors are then fabricated by embedding these chiroptically active fibers into elastomeric films. The chiroptical response on stretching is indicated quantitatively as reversible changes in magnitude, spectral position (wavelength), and sign in circular dichroism (CD) and linear dichroism (LD) signals and qualitatively as a prominent change in the birefringence features under cross-polarizers. The observed periodic twisted helical fibrils at the surface of fibers provide insights into the origin of the fibers' chirality. The measurable shifts in CD and LD are caused by elastic deformations of these helical fibrillar structures of the fiber. To elucidate the origin of these chiroptical properties, we used field emission-electron microscopy (FE-SEM), atomic force microscopy (AFM), synchrotron X-ray analysis, polarized optical microscopy, as well as measurements to isolate the true CD, and contributions from photoelastic modulators (PEM) and LD. Our findings thus offer a promising strategy to fabricate chiroptical strain-sensing devices with multiple measurables/observables using electric-field-assisted spinning of homochiral nano/microfibers.
Wildlife often uses a combination of colors in their skin, scales, and feathers to both attract mates and avoid predators. Some animals express an extreme level of black color, called “ultrablack” with reflectance <0.5%. The various nano/microstructures that produce ultrablack have been studied and replicated synthetically. These synthetic ultrablack materials, however, use highly advanced and costly techniques, toxic substances, and lack the flexibility and biocompatibility that are often desired in real-world textile applications. Here we show that a conventional natural fabric can be transformed into an ultrablack one with a biocompatible dye and a surface modification to create nanofibrils. The ultrablack wool fabrics we report have an average total reflectance of 0.13% ( λ = 400–700 nm) and represent the darkest fabrics currently reported. Unlike commercially available ultrablack fabrics, the ultrablack wool developed in this study remains breathable and conformable. Furthermore, it exhibits wide-angle ultrablack performance, maintaining a symmetric (angle-independent) optical response across a 120° angular span. Environmental and mechanical tests also prove the material’s resilience, showing the retention of its natural fabric characteristics alongside its ultrablack properties. To demonstrate the manufacturability in the textile industry, we present multiple parameter sets for plasma etching to achieve the ultrablack effect.
Many adsorbent materials are being studied for dye and oil removal from the environment. Bio-based materials such as silk are promising candidates due to their enhanced affinity for dyes and intrinsic hydrophobicity. This work extensively studies various silk textiles as dye and oil adsorbents. For comparison, we use electrospun fiber mats and hollow silk microparticle-treated silk fabrics. Our work is motivated by two factors: (i) massive amounts of silk waste is being discarded annually from textile factories, and (ii) the limited studies on the adsorption phenomena of pristine silk textiles. Based on our findings, 12 mg of silk filament yarn has a 90% methylene blue (MB) removal efficiency within 10 min of exposure for concentrations up to 100 ppm and exhibits adsorption capacities of 145 mg/g for 800 ppm concentrations. The adsorption kinetics obey a pseudo-second order, where the rate-controlling step is chemisorption, and isotherms follow the Langmuir model with homogenous monolayer adsorption. Furthermore, noil woven fabrics with contact angles of 1400 have oil adsorbent capacities that are double the fabric weight. Our work confirms that silk waste textiles are efficient and reusable bio-adsorbents for MB dye and oil removal, outperforming materials made with additional and energy-intensive techniques such as silk dissolution and electrospinning.
Interfacial solar vapor generation (ISVG), which harnesses sunlight for water distillation, presents a promising strategy to address global water scarcity. While conventional 3D evaporators offer high evaporation performance, their widespread implementation remains constrained by material selection, cost, and fabrication methods. Herein, we present a nature‐inspired, polydopamine (PDA)‐dyed wool textile as a 2.5D evaporator for ISVG, leveraging its double‐sided evaporating surfaces to maximize overall evaporation performance. The inherent fibrous architecture of wool textiles enables efficient water transport via natural capillary and exhibits effective solar absorption through photothermal PDA dyeing. The hierarchical nanostructure on micro‐scale fibers, created by subsequent plasma etching, further amplifies the light trapping and moisture wicking capabilities. Under 1‐Sun illumination, the PDA‐wool and ultrablack PDA‐wool textiles achieve evaporation rates of 2.21 and 2.43 kg/m 2 /h, respectively. In modeled calculations, both outperform the commercial baseline, with ultrablack‐wool exceling in low‐solar regions. The all‐natural composition eliminates concerns regarding the leaching of microplastics or hazardous nanomaterials. Furthermore, the system maintains a stable evaporation rate for 10 h of continuous operation without salt‐accumulation. This approach opens new opportunities for natural textiles and offers a cost‐effective route toward deployment of textile‐based solar‐driven water purification systems with strong practical viability in off‐grid and socially vulnerable communities.
Polydopamine (PDA)‐dyed wool textiles offer a potentially scalable route to ultrablack materials that combine wide‐angle reflectance suppression, flexibility, breathability, and biocompatibility. Their development, however, has remained largely empirical, lacking structural and mechanistic foundations for PDA dyeing, and prior ultrablack wool systems have been restricted to merino‐based single‐jersey fabrics. Here, we establish a multimodal structural and mechanistic framework for PDA dyeing by integrating dopamine polymerization chemistry, fiber surface chemistry and ultrastructure, as well as macroscopic fabric architecture. These factors collectively govern dye uptake and optical response. Dye formulation optimization reduces the dyeing time to 15–30 min across merino and generic wool fibers spanning diverse fabric architectures. Notably, fabric architecture emerges as a dominant design variable for controlling wide‐angle optical response, a previously underappreciated lever for engineering photonic textiles. Mechanistic analysis of dopamine polymerization reveals PDA formation in wool as an absorption‐driven dyeing process rather than a purely surface‐coating process, whose uptake and interactions within the porous fibrous matrix contribute to near‐zero reflectance when plasma‐treated. Together, these findings provide a material design blueprint for scalable ultrablack wool textiles and offer broader principles for flexible photonic devices.