Polyolefin is the most widely used and versatile commodity polymer. In this work, three types of polyolefin-based elastomers (PBEs) were adopted to toughen a high-flow polypropylene to improve its overall performance. The chain microstructures of these PBEs, including ethylene/1-octene (E/O) random copolymer from Dow Chemical′s polyolefin elastomer (POE), olefin block copolymers (OBCs) of E/O from Dow, and ethylene/propylene random copolymer from ExxonMobil’s propylene-based elastomer, were elucidated by GPC, 13C NMR, TREF, and DSC techniques. The mechanical, thermal and optical properties, and morphology analysis of the PP/PBE blends were also studied to investigate the toughening mechanism of these PBEs. The results showed that all three types of PBEs can effectively improve the Izod impact strength of the PP/PBE blends by the addition of the rubber compositions, at the cost of the stiffness. PBE-1 and PBE-2 were found to have a great stiffness–toughness balance with about 1700 MPa of flexural modulus, about 110 °C of HDT and 3.6 kJ/m2 of impact strength on the prepared PP/PBE blends by forming separated rubber phase and refined spherulite crystals. As a result, the OBC with alternating hard and soft segments could achieve a similar toughening effect as the E/P random copolymer. Surprisingly, no obvious rubber phase separation was observed in the PP/PBE-4 blend, which might be due to the good compatibility of the E/P random chains with the isotactic PP; therefore, the PP/PBE blend obtains great toughness performance and optical transparency with the highest Izod impact strength of 4.2 kJ/m2 and excellent transparency.
Porous organic polymers (POPs) have received much attention in adsorption, separation, and catalysis. In this paper, porous organic polymers with different pore structure were used as metallocene catalyst supports, and ethylene/1-hexene copolymerizations were conducted using the POPs-supported metallocene catalyst. The pore structure of the prepared POPs and the supported metallocene catalyst were characterized by nitrogen sorption porosimetry and non-local density functional theory simulation, and the molecular chain structure of the produced ethylene/1-hexene copolymers were investigated through gel permeation chromatography (GPC), IR analysis, differential scanning calorimetry (DSC), and temperature rising elution fractionation (TREF). The results show that the loading amount of active sites varied with different pore structures of the POP supports, and the active species scattered in different pore sizes had a moderate impact on the molecular chain growth and the molecular weight distribution. The IR, DSC, and TREF analysis revealedthat different branching degree, double bond content, and chemical composition distributions were detected from the molecular chain structure of the ethylene/α-olefin copolymers from different POPs and silica-supported metallocene catalysts, despite their similar IR, DSC, and TREF curves due to the same active species. Scanning electron microscopy (SEM) showed that porous ethylene/α-olefin copolymers with varied surface morphology were obtained from the POPs-supported metallocene catalysts with different pore structure.
The stereospecific polymerization of 1-alkenes is a continuing issue for metal catalysis. We have initially reported isoselective 4-methylpentene polymerizations by nonconventional pyridylamido hafnium catalysts with different bridgehead substituents (L(R1R2)Hf(Me)2, L = pyridylamido; 1: R1 = 2-iPr–Ph, R2 = H; 2: R1 = tBu, R2 = H; 3: R1 = R2 = Me). The effects of polymerization temperature, monomer concentration, and bridgehead substituents were systematically investigated. Regardless of the bridgehead substituent and polymerization temperature, highly isotactic poly(4-methylpentene)s (PMPs) ([mmmm] > 99%) with high melting temperatures (Tm = 229–240 °C) were produced. The bridgehead substituents of pyridylamido hafnium catalysts remarkably affected the polymerization activity and molecular weight distribution (MWD) of the resultant PMPs. Catalyst 1 showed much higher activity (14 500 kg PMP (mol Hf h)−1) than catalysts 2 and 3. PMPs produced by catalyst 2 displayed unimodal distributions (MWD = 3.0–4.7), but polymers produced by catalysts 1 and 3 had clear bimodal distributions (MWD > 10). Besides, X-ray powder diffraction clearly showed that crystalline forms of the resultant PMPs were dependent on the polymerization temperature and catalyst structure.
Polypropylene (PP) is one of the most widely used polymers. In this paper, three types of PPs including random PP, impact PP, and impact PP with high clarity, were prepared through a 75 kg/h pilot-scale Spheripol II process. The three produced PPs were produced by the selection or combination the two loops and gas phase reactor and controlling the comonomer and hydrogen concentrations. The three prepared PPs then were pelleted with the clarified nucleating agent NX 8000 and tested for mechanical, thermal, and optical properties. Their molecular structures and rubber phase size were also investigated by GPC, 13C NMR, temperature rising elution fractionation (TREF), XRD, SEM analysis, etc. The results showed that the random PP (PP-1) and the impact PP with high clarity (PP-3) obtained excellent optical transparency with a haze of 12.5% and 13.5% due to their small rubber phase size (roughly ≤ 100 nm), while the impact PP (PP-2) obtained bad transparency with a haze of 98.8% due to the large rubber phase size (about 1 μm) caused by the poor thermal compatibility with the PP matrix. The rubber phase content and ethylene/propylene sequence distributions of the three PPs varied much and resulted in different impact strengths and stiffness properties. PP-2 had a high impact strength of 14.5 kJ/m2 due to the rubber phase generated in the gas phase reactor. Except for the optical transparency, PP-3 gained stiffness and toughness, with 914 MPa of flexural modulus and 25.1 kJ/m2 of impact strength due to the unique molecular structure of its rubber phase.