During the thermal treatment of kaolinite, the main mineral phase in kaolin rock, dehydroxylation occurs, forming metakaolin through a process that has significant industrial applications. This study experimentally analyzed dehydroxylation in two kaolinite samples: a well-crystallized reference sample from the Clay Mineral Society and a locally sourced, industrial kaolin sample. The mechanism and kinetic parameters were evaluated from a series of thermogravimetric measurements. Non-isothermal kinetic analysis revealed that dehydroxylation followed a third-order (F3) reaction mechanism, with activation energies () ranging from 35 to 60 kcal/mol. Additionally, theoretical calculations based on Density Functional Theory were performed on four systems in which a water molecule was removed by combining OH group and H atom vacancies in the kaolinite unit cell. These models represented the onset of dehydroxylation and provided values for the reaction energy Q from first-principles calculations, which served as reference values for . The results confirm that water molecule formation involving both OH at the kaolinite outer surface and inner surface are energetically competitive and highlight the crucial role of structural relaxations following water removal to determine Q values in the range of 30–50 kcal/mol, in very good agreement with the experiments.
This study investigates the thermal shock behavior of three Al2O3-SiO2 commercial insulating refractory materials (JM23, JM26, and JM28) used in high-temperature industries (>1000 °C). Thermal shock resistance was evaluated through experimental tests and compared with theoretical parameters (R, R⁗, Rst) based on thermoelastic and thermomechanical models. The tests revealed that JM23 did not withstand thermal shock due to its fragility when in contact with water at room temperature, resulting in its immediate collapse. In contrast, JM26 and JM28 maintained their mechanical strength after several thermal shock cycles, although JM28 experienced a more significant decrease in compressive strength. The mechanical behavior under compression changed from semi-fragile to apparently plastic after severe heat treatments. Porosity analysis showed that JM26 had a lower pore size distribution, which contributed to its better thermal shock performance. Theoretical parameters were calculated, confirming that JM26 exhibited the highest resistance to thermal shock. These findings suggest that controlled porosity and microstructure are key factors in improving the thermal performance and durability of insulating refractory materials in high-temperature applications.
6 October 2024 in International Journal of Applied Ceramic Technology