Fe78Si9B13 amorphous particles with high saturation magnetization, low remanence and low coercivity are applied in preparing magnetorheological fluids.
Magnetic Fe-B, Fe-Ni-B, and Co-B nanoparticles were successfully synthesized and introduced to water to prepare aqueous ferrofluids. The Fe-B, Fe-Ni-B, and Co-B particles are homogeneous amorphous nanoparticles with an average particle size 15 nm. The shape of the amorphous nanoparticles is regular. The Fe-B, Fe-Ni-B, and Co-B amorphous nanoparticles are superparamagnetic. Moreover, the saturation magnetizations of Fe-B and Fe-Ni-B amorphous nanoparticles are 75 emu/g and 51 emu/g. These are approximately 2.8 and 1.9-fold larger than Co-B nanoparticles, respectively. The viscosity of the amorphous ferrofluids has a strong response to external magnetic field. The yield stress increases with increasing magnetic field. The hyperthermia research of amorphous ferrofluids was firstly investigated. The experimental results indicate that the heating temperature of Fe-B ferrofluid and Fe-Ni-B ferrofluid could increase to 42 °C in 750 s and 960 s, respectively, when the output current is 300 A. The temperature could reach 61.6 °C for a Fe-B ferrofluid. The heating efficiencies of the amorphous ferrofluids demonstrate that the Fe-B ferrofluid and Fe-Ni-B ferrofluid may have great potential for biomedical applications.
A novel magnetic fluid was obtained using a colloidal dispersion of amorphous magnetic Fe-Ni-B nanoparticles into water. Its magnetorheological and viscoelastic behaviors were all investigated. Results showed that the generated particles were spherical amorphous particles 12–15 nm in diameter. The saturation magnetization of Fe-based amorphous magnetic particles could reach 49.3 emu/g. The amorphous magnetic fluid exhibited shear shinning behavior under magnetic fields and showed strong magnetic responsiveness. The yield stress increased with the rising magnetic field strength. A crossover phenomenon was observed from the modulus strain curves due to the phase transition under applied magnetic fields. The storage modulus G′ was higher than the loss modulus G″ at low strains, while G′ was lower than G″ at high strains. The crossover points shifted to higher strains with increasing magnetic field. Furthermore, G′ decreased and fell off in a power law relationship when the strain exceeded a critical value. However, G″ showed a distinct maximum at a critical strain, and then decreased in a power law fashion. The magnetorheological and viscoelastic behaviors were found to be related to the structural formation and destruction in the magnetic fluids, which is a joint effect of magnetic fields and shear flows.