This study is the first to research the microstructure and mechanical properties of the workpiece after additive friction stir deposition (AFSD) of the feedstock at different heat treatment stages. AA2219 aluminum alloys with three different heat treatment stages were selected as the feedstock, and alloys with dense structure were successfully prepared by the additive friction stir deposition AFSD process. Experimental results show that AFSD exhibits an excellent ability to refine grains and improve the uniform distribution of precipitates in the second phase, thereby improving the plasticity of AA2219 alloy after the AFSD process. Because of the continuous dynamic recrystallization (CDRX) in the AA2219 alloy during AFSD, the grain size after the AFSD process is independent of the initial feedstock grain size for three samples. The equilibrium phase (θ) size is genetically related to the initial size of the second-phase particles in the feedstock. Due to grain refinement and dislocation strengthening, the yield strength of AA2219-casting increased significantly from 79.8 MPa to 124.1 MPa after AFSD. The yield strength of the AA2219-T4 decreases slightly from 151.8 MPa to 140.4 MPa after AFSD. The precipitation of the second phase leads to a decrease in solid solution strengthening and dislocation strengthening. However, grain refinement strengthening partially offsets this reduction. The yield strength of AA2219-T87 decreased from 398.5 MPa to 147.2 MPa after AFSD. As such, grain refinement strengthening and solid solution strengthening by the AFSD process are much smaller than the yield strength lost by precipitation strengthening and dislocation strengthening.
29 July 2024 in The International Journal of Advanced Manufacturing Technology
In this study, composite plates of 6061/TA1 were successfully manufactured using additive friction stir deposition (AFSD). The impact of preheating temperatures (room temperature, 100 °C, 200 °C) on the interfacial microstructure and interface mechanical properties at various deposition zones was studied. The results showed that as the preheating temperature increased or when the deposit zone shifted from the boundary to the center, the diffusion width of Al and Ti increased, accompanied by an increase in bonding shear strength. Moreover, in the boundary zone of the sample preheated at room temperature (P-RT), only mechanical bonding was observed, resulting in the lowest bonding shear strength. Conversely, the other samples exhibited a combination of mechanical and metallurgical bonding. Under the preheating temperature of 200 °C, interfacial intermetallic compounds were observed near the center zone, which exhibited the highest bonding shear strength.
The fabrication of multi-layer alloys by additive friction stir deposition (AFSD) results in a complicated microstructure and mechanical property evolution due to the repeated thermal inputs impacting the existing deposited layers. This work systematically studied the microstructure and mechanical properties of several areas (last layers, intermediate layers, and first layers) of a 16-layer 2195 alloy component fabricated by AFSD to ascertain the effect of repeated thermal cycling. The periodic heat input resulted in the minimal quantities of T1-phase only appearing in the last layers of the sample, while the θ′-phase developed a complex precipitate with the δ′ and β′ phases. The mechanical properties of the 2195 sample exhibit a gradient development related to the microstructure, with a decrease in strength and hardness from top to bottom. The samples located in the last layers show the highest microhardness of 117.0 Hv, yield strength of 296.6 MPa, ultimate tensile strength of 440.6 MPa, and elongation of 27.1%, respectively.
15 February 2025 in Progress in Additive Manufacturing
In this work, the oxidation behavior of an aluminide coating at 900, 1000, and 1100 °C was investigated. The aluminide coating was prepared on a cobalt-based superalloy using a vapor phase aluminizing process, which is composed of a β-(Co,Ni)Al phase outer layer and a Cr-rich phase diffusion layer. The experimental results showed that the oxidation of the coating at 900–1100 °C all obey the parabolic law. The oxidation rate constants of the coating were between 2.19 × 10−7 and 47.56 × 10−7 mg2·cm−4·s−1. The coating produced metastable θ-Al2O3 at 900 °C and stable α-Al2O3 at 1000 and 1100 °C. As the oxidation temperature increases, the formation of Al2O3 is promoted, consuming large amount of Al in the coating, resulting in the transformation from β-(Co,Ni)Al phase to α-(Co,Ni,Cr) phase. And the decrease in the β phase in the coating led to the dissolution of the diffusion layer.