To exploit the whole potential of Additive Manufacturing, it is essential to investigate the complex relationships between Additive Manufacturing processes, the resulting microstructure, and mechanical properties of the materials and components. In the present work, Selective Laser Melted (SLM) (process category: powder bed fusion), Laser Deposition Welded (LDW) (process category: direct energy deposition) and, for comparison, Continuous Casted and then hot and cold drawn (CC) austenitic stainless steel AISI 316L blanks were investigated with regard to their microstructure and mechanical properties. To exclude the influence of surface topography and focus the investigation on the volume microstructure, the blanks were turned into final geometry of specimens. The additively manufactured (AM-) blanks were manufactured in both the horizontal and vertical building directions. In the horizontally built specimens, the layer planes are perpendicular and in vertical building direction, they are parallel to the load axis of the specimens. The materials from different manufacturing processes exhibit different chemical composition and hence, austenite stability. Additionally, all types of blanks were heat treated (2 h, 1070 °C, H2O) and the influence of the heat treatment on the properties of differently manufactured materials were investigated. From the cyclic deformation curves obtained in the load increase tests, the anisotropic fatigue behavior of the AM-specimens could be detected with only one specimen in each building direction for the different Additive Manufacturing processes, which could be confirmed by constant amplitude tests. The results showed higher fatigue strength for horizontally built specimens compared to the vertical building direction. Furthermore, the constant amplitude tests show that the austenite stability influences the fatigue behavior of differently manufactured 316L. Using load increase tests as an efficient rating method of the anisotropic fatigue behavior, the influence of the heat treatment on anisotropy could be determined with a small number of specimens. These investigations showed no significant influence of the heat treatment on the anisotropic behavior of the AM-specimens.
1 February 2020 in International Journal of Fatigue
The 22 wt.% Cr, fully ferritic stainless steel Crofer®22 H has higher thermomechanical fatigue (TMF)- lifetime compared to advanced ferritic-martensitic P91, which is assumed to be caused by different damage tolerance, leading to differences in crack propagation and failure mechanisms. To analyze this, instrumented cyclic indentation tests (CITs) were used because the material’s cyclic hardening potential—which strongly correlates with damage tolerance, can be determined by analyzing the deformation behavior in CITs. In the presented work, CITs were performed for both materials at specimens loaded for different numbers of TMF-cycles. These investigations show higher damage tolerance for Crofer®22 H and demonstrate changes in damage tolerance during TMF-loading for both materials, which correlates with the cyclic deformation behavior observed in TMF-tests. Furthermore, the results obtained at Crofer®22 H indicate an increase of damage tolerance in the second half of TMF-lifetime, which cannot be observed for P91. Moreover, CITs were performed at Crofer®22 H in the vicinity of a fatigue crack, enabling to locally analyze the damage tolerance. These CITs show differences between crack edges and the crack tip. Conclusively, the presented results demonstrate that CITs can be utilized to analyze TMF-induced changes in damage tolerance.
For a reliable design of structural components, valid information about the fatigue strength of the material used is a prerequisite. As the determination of the fatigue properties, and especially the fatigue limit σw, requires a high experimental effort, efficient approaches to estimate the fatigue strength are of great interest. Available estimation approaches using monotonic properties, e.g., Vickers hardness (HV), and in some cases the cyclic yield strength, only allow a rough estimation of σw. The approaches solely based on monotonic properties lead to substantial deviations of the estimated σw in relation to the experimentally determined fatigue limit as they do not consider the cyclic deformation behavior. In this work, an estimation approach was developed, which is based on a correlation analysis of the fatigue limit σw, HV, and the cyclic hardening potential obtained in instrumented cyclic indentation tests (CIT). For this, eleven conditions from five different low-alloy steels were investigated. The CIT enable an efficient and quantitative determination of the cyclic hardening potential, i.e., the cyclic hardening exponentCHTeII, and thus, the consideration of the cyclic deformation behavior in an estimation approach. In this work, a strong correlation of σw with the product of HV and |eII| was observed. In relation to an existing estimation approach based solely on HV, considering the combination of HV and |eII| enables the estimation of σw with an enormously increased precision.