To curtail the negative effects of traditional flood machining, dry cutting using carbide tools has emerged as a prominent alternative for manufacturers, owing to its low cost and phenomenal surface qualities. In line with this view, high-speed machining of high-strength AISI 4340 alloy steel was carried out using multilayer Al2O3/TiCN-CVD and TiAlN/AlCrN-PVD carbide tools in a dry environment. The experimental scheme was adopted, as per Taguchi’s L18 orthogonal array, to investigate the two most crucial machinability aspects, namely tool life and surface roughness. An analysis of variance (ANOVA) was performed on the obtained data, and it was inferred that the feed rate exhibited the strongest effects on both the tool life and surface roughness, with corresponding percentage contributions of 46.22% and 68.96%, respectively. The longest tool lives of 14.75 min and 10.08 min were obtained at a low cutting speed and feed rate for CVD and PVD tools, respectively. However, the lowest surface roughness of 0.276 µm and 0.307 µm was achieved at a high cutting speed and low feed rate for PVD and CVD tools, respectively. The evolution of tool wear, studied through the microscopic images of the worn tools, revealed that a high cutting speed and feed rate accelerated the flank wear for both types of tools. Nevertheless, the CVD tool exhibited better results due to the thick and effective Al2O3/TiCN coating layer, which protected the carbide substrate against thermal–mechanical loads. Moreover, scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDX) performed on the worn tools revealed that adhesion, oxidation, diffusion, and abrasion were the main wear mechanisms for both types of tools.
Hard turning is a precision machining process used to cut materials with hardnesses exceeding 45 HRC using single-point tools. It offers an efficient alternative to traditional grinding for finishing operations in manufacturing. This paper explores the machinability of hardened AISI 4340 steel for a hard turning process utilizing dry and cryogenic (Cryo) plus minimum quantity lubrication (MQL) (Cryo+MQL) techniques, focusing on critical machinability aspects such as cutting force, surface roughness, and tool life. The orthogonal dry turning was performed with a cutting speed (V) ranging from 300–400 m/min, a feed rate (f) between 0.05 and 1 mm/rev, and a depth of cut (doc) from 0.1 to 0.3 mm. A statistical analysis of the obtained results revealed that the feed rate was the most influential parameter, contributing 50.69% to the main cutting force and 80.03% to surface roughness. For tool life, cutting speed was identified as the dominant factor, with a contribution rate of 39.73%. Multi-objective optimization using Grey relational analysis (GRA) identified the optimal machining parameters for the hard turning of AISI 4340 alloy steel as V = 300 m/min, f = 0.05 mm/rev, and doc = 0.1 mm. The Cryo+MQL technique was subsequently applied to these parameters, yielding significant improvements, with a 48% reduction in surface roughness and a 184.5% increase in tool life, attributed to enhanced lubrication and cooling efficiency. However, a slight 4.6% increase in cutting force was observed, likely due to surface hardening induced by the low-temperature LN2 cooling. Furthermore, reduced adhesion and tool fracture on the principal cutting edge under Cryo+MQL conditions justify the superior surface quality and extended tool life achieved. This research highlights the industrial relevance of hybrid lubrication in addressing challenges associated with hard turning processes.
The fabrication of bi-material micro-components via two-component micro-powder injection moulding (2C-µPIM) from 3 mol% yttria-stabilised zirconia (3YSZ) and micro/nano bimodal stainless steel 316L (SS 316L) powders has received insufficient attention. Apart from this, retaining the bonding between ceramic and metal at different processing stages of 2C-µPIM is challenging. This study investigated the solvent and thermal debinding mechanisms of green bi-material micro-parts of 3YSZ and bimodal SS 316L without collapsing the ceramic/metal joining. In this research, feedstocks were prepared by integrating the powders individually with palm stearin and low-density polyethylene binders. The results demonstrated that during the solvent debinding process, the palm stearin removal rate in the bi-materials composed of 3YSZ and bimodally configured SS 316L feedstocks intensified with an increase in temperature. The establishment of interconnected pores in the solvent-debound components facilitated the thermal debinding process, which removed 99% of the binder system. Following sintering, the debound bi-materials exhibited a relative density of 95.3%. According to a study of the microstructures using field emission scanning electron microscopy, an adequate bond between 3YSZ and bimodal SS 316L was established in the micro-part after sintering. The bi-material sintered at 1350 °C had the highest hardness of 1017.4 HV along the joining region.
Two-component micro-powder injection moulding (2C-μPIM) is a prospective approach for fabricating bi-material micro-components of stainless steel 316L (SS316L) and 3 mol% yttria-stabilised zirconia (3YSZ) at an appealing cost. However, the fundamental challenge lies in preventing the formation of large-scale cracks at the interface of two different materials during sintering. This study investigated how SS316L nanoparticles in bimodally configured SS316L powder that incorporated both nanoparticles and microparticles influenced the sintering of 2C-μPIM-processed miniature bi-materials made of bimodal SS316L and 3YSZ. In this study, feedstocks were developed by integrating monomodal (micro-sized) SS316L powder, three types of nano/micro-bimodal SS316L powders, and 3YSZ powder individually with palm stearin and low-density polyethylene binders. The results indicated that increasing the SS316L nanoparticle content to 45 vol.% caused a 19.5% increase in the critical powder loading in the bimodal SS316L powder as compared to that in the monomodal SS316L powder. The addition of SS316L nanoparticles increased the relative density and hardness of the sintered bi-materials, with the maximum values obtained being 96.8% and 1156.8 HV, respectively. Field emission scanning electron microscopy investigations revealed that adding 15 vol.% and 30 vol.% SS316L nanoparticle contents reduced interface cracks in bi-materials significantly, while 45 vol.% resulted in a crack-free interface.
16 February 2026 in Journal of Materials Engineering and Performance