This study examines the preservation challenges of archaeological iron, bone, and glass within shared environments focusing on material-specific degradation mechanisms. The relative humidity (RH) requirements for these materials can vary significantly. Iron presents distinct stability groups at specific RH thresholds, albeit levels below 30% RH are recommended for sensitive artefacts. Little is known about the moisture response of bone, and the heterogeneity of the material poses additional challenges for its examination. Glass can undergo deterioration at both high and low RHs due to the threat of aqueous attack and transformation of the pristine glass or the crizzling and delamination of the already transformed glass. Experiments employing dynamic vapour sorption (DVS), acoustic emission (AE), and oxygen depletion analyses provided insights into the moisture response behaviours of these materials. It was found that the deleterious akageneite formation increases dramatically at RHs > 30% in archaeological iron, reinforcing the current guidelines. Bone exhibits significant hygroscopicity as well as isotherm steepening below 25% RH on desorption, suggesting this threshold could be advisable to avoid structural damage. In glass, there is evidence of significant mass fluctuations between c. 60 and 95% RH, as well as isotherm steepening around 30% RH on desorption, thus providing more empirical evidence to published storage recommendations. This work sheds more light on the risk assessment for mixed-material showcases and underscores the necessity of nuanced RH guidelines that consider the material-specific degradation mechanisms.
Maintaining a tight RH range for unstable glass is energy- and carbon-intensive. The carbon footprint of several methods for controlling showcases and storerooms, including sorbents, dehumidifiers and sorbents, Miniclima, and RK2, has been measured. Dehumidifiers outperformed Miniclima and RK2 units in control capability, but all three exhibited a higher carbon footprint than passive control methods. However, tailoring the right conditions for the right objects is crucial. The decay of different glass compositions in atmospheric conditions was measured using surface ion swabbing. Conditions below 40% in addition to forced air movement universally slowed deterioration. Formic acid was found to significantly accelerate glass alteration but could be removed using the RK2 unit.
A survey of current damage functions for assessing data from material and environmental control perspectives. When conservation and preservation professionals are asked to consider the impact of changes related to collection environments, buildings, and energy consumption, damage functions support risk assessment activities and inform decisions. The damage functions highlighted include chemical deterioration of paper, TWPI, isoperm and modern, mould growth, mechanical damage of wood, tarnish rate of silver, corrosion of copper, physical damage to stone via salts, pest activity, and corrosion of archaeological metals, among others.