Borosilicate glass was developed to enhance the mechanical behavior and smoothness of dental zirconia as an alternative to conventional glaze. This study assessed the mechanical and optical properties of 3 mol% yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) coated with borosilicate glass or a commercial glaze fired for an extended period of time. Disc-shaped 3Y-TZP zirconia specimens (Zpex, Tosoh) were sintered at 1550°C for 2 hours. The specimens were divided into three groups: as-sintered (control, C); commercial glaze (G); and borosilicate glass (SL). The glaze and borosilicate glass were applied over the zirconia and fired for 20 minutes at 950°C and 1200°C, respectively. Biaxial flexural strength, fractography, X-ray diffraction (XRD), roughness (Ra and Rz), fracture toughness (Vickers indentation method), color difference (∆E00), and translucency (TP00) analyses were conducted. The t-test or the one-way ANOVA and Tukey’s tests were used to analyze the data (α = 0.05). Flexural strength data were subjected to the Weibull analysis. The SL group exhibited the highest flexural strength (1025.8 MPa), whereas the C (859.41 MPa) and G (816.0 MPa) groups exhibited similar values. The SL group also had the highest characteristic strength. The fracture origin in all groups was on the zirconia surface. XRD analysis revealed that the specimens from the SL group contained tetragonal, cubic, and monoclinic phases. The SL group presented the lowest surface roughness. Fracture toughness in the SL group was lower than in the C group, but similar to that observed in the G group. The translucency and color differences observed in the G and SL groups were similar. Borosilicate glass enhanced the flexural strength of 3Y-TZP, promoted the smoothest surface, and exhibited optical properties similar to those of the glaze.
OBJETIVO: revisar a literatura sobre o protocolo de planejamento e diagnóstico digital conhecido como “Digital Smile Design”, destacando suas principais vantagens no tocante a reabilitações estéticas em odontologia restauradora. MATERIAL E MÉTODO: foi realizada busca nas bases de dados da Pubmed, Scielo e Bireme, de 60 artigos, utilizando os termos de busca Dental photography cosmetic dentistry, treatment protocols. Os critérios de inclusão foram: Estudos in vivo, revisões sistemáticas e metanálise, literatura que aborda variáveis em estudo, idioma em português e inglês e artigos publicados no período de 1990 a 2020. Os critérios de exclusão foram: carta ao editor, revisão de literatura e caso clínico. RESULTADOS: o DSD é uma ferramenta de planejamento de tratamento utilizada em odontologia estética interdisciplinar para fortalecer a visão diagnóstica, melhorar a comunicação entre especialistas e a orientação do paciente. O design do sorriso se refere aos muitos princípios científicos e artísticos que, coletivamente, podem criar um belo sorriso. Esses princípios são estabelecidos por meio de dados coletados dos pacientes como modelos diagnósticos, anamnese e medida de proporções faciais. Por sua vez, a composição estética do sorriso depende de muitos pontos de referência e parâmetros anatômicos para a formação de um conjunto harmônico e belo. CONSIDERAÇÕES FINAIS: o DSD é uma ferramenta importante para uso em reabilitações estéticas em odontologia restauradora, uma vez que é um instrumento facilitador do diagnóstico, melhora a comunicação entre a equipe multidisciplinar e auxilia na orientação e motivação do paciente, aumentando a previsibilidade dos tratamentos.
A 5Y‐PSZ zirconia paste was formulated for extrusion‐based additive manufacturing via Direct Ink Writing (DIW) to produce dense ceramic components for dental applications. A colloidal approach was adopted using nanometric zirconia powder (47 vol%) with tailored dispersant, thickener, and flocculant agents. Rheological behavior was evaluated by shear viscosity, viscoelastic moduli, and three‐step thixotropy tests to ensure printability and shape stability. Specimens were printed with different filament overlap percentages (20%, 25%, and 30%) and compared with a control group obtained by uniaxial pressing. After sintering, all groups were characterized in terms of relative density, microstructure (SEM), phase composition (XRD), translucency, and biaxial flexural strength. The 30% overlap printed group achieved average densification above 99%, optical translucency comparable to the pressed controls, and flexural strength of 432 ± 37 MPa. Weibull analysis of 30% filament overlap group indicated σ 0 = 420 MPa and m = 7.0, comparable to the pressed group (σ 0 = 658 MPa; m = 7.3). Overall, this study establishes a robust formulation and processing route for DIW of 5Y‐PSZ with high densification, translucency, and mechanical reliability, fulfilling ISO 6872 and offering a viable alternative for dental applications. This is the first study demonstrating filament overlaps as a densification‐enhancing parameter for DIW zirconia.
Acrylic resin is widely used in the fabrication of complete dentures, interacting significantly with the intraoral environment. However, complete dentures face challenges such as stability issues and biofilm accumulation. Glaze application is a common method to reduce surface porosity and microbial adhesion, but it also decreases surface wettability, potentially impairing salivary film formation essential for peripheral sealing. This study aimed to incorporate titanium dioxide and zinc oxide nanoparticles into the glaze applied to thermally activated acrylic resin (TAAR) via spray coating to enhance surface wettability and antifungal activity. Four groups were tested: G (TAAR + commercial glaze − control); AlG (TAAR + commercial glaze + aluminum oxide − roughness control); TiG (TAAR + commercial glaze + titanium dioxide); and ZnG (TAAR + commercial glaze + zinc oxide). Evaluations included flexural strength, color and translucency, surface analysis and antibiofilm activity against Candida albicans. Data were analyzed using one-way ANOVA. No statistically significant differences in mechanical strength (MPa) were observed (G: 108.54 ± 8.36; AlG: 113.60 ± 11.95; ZnG: 111.98 ± 9.27; TiG: 113.66 ± 10.41). Surface roughness significantly increased, and contact angle decreased, indicating improved wettability. Regardless of the antifungal activity no improvement was detected (G: 6.71 ± 0.10; AlG: 6.82 ± 0.08; ZnG: 6.72 ± 0.20; TiG: 6.66 ± 0.18). In conclusion, the incorporation of nanoparticles into the glaze improves the wettability of acrylic resin surfaces, potentially enhancing peripheral sealing and denture retention, which is beneficial for patients with reduced alveolar ridge height.