Nano aluminum powders and nano-ZrO2 reinforcement particles were mechanically milled and hot?pressed to produce Al-ZrO2 nanocomposites. Microstructure and mechanical properties of Al-ZrO2 nanocomposites were investigated using SEM, EDX, and XRD analysis and by performing hardness and compression testing. Uniform particle distribution could be obtained up to 3 wt.% of nano-ZrO2 particles by using nano-sized aluminum powders as matrix powders and by applying a mechanical milling process. As the nano-ZrO2 reinforcement particles were uniformly distributed in the matrix, the relative density of the Al-ZrO2 nanocomposites increased up to 3 wt.% nano-ZrO2 particles with an increase in milling time; on the other hand, the relative density decreased and the porosity increased with high-weight fractions (>3wt.%) of nano-ZrO2 particles due to the negative combined effect of less densification and an increase in the number of particle clusters. The hardness and compressive strength of the Al-ZrO2 nanocomposites could be improved despite increased porosity. On the other hand, the compressive strength of Al-ZrO2 nanocomposites with a high amount (>3 wt.%) of nano-ZrO2 particles has begun to decrease due to the negative combined effect of the less densification of the powder-particles and the clustering of nano-ZrO2 reinforcement particles. The brittle-ductile fracture occurred in the Al-ZrO2 nanocomposites.
15 April 2022 in International Journal of Materials Research
The tensile responses of three monolithic composites (aramid, carbon, and glass) and three different interply hybrid composite laminates (aramid/carbon, glass/aramid, and glass/carbon) were studied at quasi-static and intermediate strain rates. Monolithic composites were found to be more sensitive to strain rate than hybrid counterparts. The hybrids with glass layers had the highest sensitivity among the hybrid laminates. Tensile strengths of aramid, carbon, and glass monolithic composites improved by 15.2 %, 10.1 %, and 22.2 %, respectively, as the strain rate was increased from 0.001 s−1 to 10 s−1, while increases in tensile strengths of aramid/carbon, glass/aramid and glass/carbon hybrid laminates were 8.8 %, 17.7 %, and 5.2 %, respectively. Hybridization of glass with aramid gave the highest failure strain gain. Carbon layers located at the centre of the hybrid laminates resulted in increased tensile strength.
This study aims to enhance the electrical conductivity of commercially pure aluminium by minimizing impurities and grain boundaries in its microstructure, ultimately improving the efficiency of electric motors constructed from rotors with squirrel cages made from this material. For this purpose, an aluminium–boron (AlB8) master alloy was added to aluminium with a purity of 99.7%, followed by the application of a grain-coarsening heat treatment to the rotors. To obtain commercially pure aluminium with boron additions of 0.05% and 0.1% by weight, specific amounts of the AlB8 master alloy were added into aluminium with a purity of 99.7%. Using these materials, squirrel cage components of rotors were produced via the high-pressure die-casting method. Subsequently, a grain-coarsening heat treatment of the rotors was performed at temperatures of 450 °C, 500 °C, and 550 °C, with holding times of 2, 6, and 10 h. The Box–Behnken design, which is based on statistical experimental design and response surface methodology, was employed to investigate the effects of adding boron and varying the heat treatment temperature and holding time on the electrical conductivity of commercially pure aluminium. The results showed that the synergistic effect of adding boron at 0.05 wt.% and applying the grain-coarsening heat treatment at a temperature of 550 °C for a holding time of 10 h significantly enhanced the electrical conductivity of commercially pure aluminium, increasing it from 60.62% IACS to 63.1% IACS. Correspondingly, the efficiency of the electric motor increased from 90.35% to 91.53%. These findings suggest that this hybrid method not only enhances the electrical conductivity of commercially pure aluminium but also has strong potential to improve its other properties, such as thermal conductivity. This will lead to products composed of components manufactured from the materials exhibiting better performance characteristics, such as increased efficiency and extended service life. Consequently, this innovative method will contribute economically and environmentally by facilitating the manufacture of high-performance products.
11 September 2025 in International Journal of Adhesion and Adhesives
The effects of volume fraction, size, and type of reinforcement particles on the microstructure and mechanical properties of Al–Si–Cu–(Fe) alloy matrix composites were investigated and an analytical model was modified to predict the yield strength of the particle-reinforced nanocomposites. Nano- and micro-particle-reinforced Al–Si–Cu-(Fe) matrix composites (N-AMCs and M-AMCs) were manufactured by adding two different types and sizes of reinforcement particles to Al–Si–Cu–(Fe) alloys at different volume fractions using a two-step stir casting method combined with a high-energy ball milling process and a high-pressure die-casting method. Microstructural analyzes of N-AMCs and M-AMCs were performed using SEM, EDX, and XRD. The Brinell hardness test and the tensile test were carried out to determine the mechanical properties of the N-AMCs and M-AMCs. The hardness of the N-AMCs and M-AMCs was continuously enhanced by increasing the volume fraction of the reinforcement particles, while the yield strength and ultimate tensile strength of the N-AMCs and M-AMCs were improved up to 1.5 vol.% and 4 vol.% of nano-particles and micro-particles, respectively. An analytical model was modified to predict the yield strength of N-AMCs by integrating the effective volume ratio of nano-particles into each strengthening mechanism. The results predicted by the modified model reached nearly 98% agreement with the experimental results up to 1.5 vol.% of the reinforcement particles. Nano-particles had a much greater effect on strengthening mechanisms compared to micro-particles.