The temperature gradient and mismatching between the thermal expansion of the core and flange readily lead to cracks and discharges on the core surface of the dry‐type valve‐side bushing, which severely impact the safety of power systems. It is vital to clarify the cracking risk of bushing cores under temperature gradients and establish corresponding control methods. The mechanical properties of epoxy resin impregnated paper (ERIP) material were measured in this study at different temperatures, and a thermal–mechanical coupling simulation model was established. The thermal and stress distributions of the core were obtained and the cracking risk was defined accordingly. The crack development mode was explored as it relates to the phase‐field mode. Various elastic cushion materials affecting the stress distribution of the core were investigated. The results show that the mechanical properties of the ERIP material decrease rapidly as the temperature increases. When under severe working conditions, the maximum first principal stress of the core may be significantly higher than the tensile strength of the ERIP material resulting in significant axial cracks. Adding an elastic cushion layer made of polyurethane rubber can effectively relax the interface stress and reduce the cracking risk.
As voltage levels increase, insulation materials have often suffered insulation failures in recent years, such as epoxy resin for valve-side bushings. Under the combined effect of strongly coupled electrothermal field, the bushing radial insulation breakdown accident happens from time to time. In this paper, an electrothermal treeing experimental setup was built. The treeing characteristics of epoxy resin from 40 to 120 °C were tested. A novel treeing model under strongly coupled electrothermal field was proposed. Treeing process based on the physical parameters was simulated by using COMSOL Multiphysics. The results show that the critical energy density of partial damage in the phase field model is determined to be 1.84×10 5 J/m 2 . The experiment and simulation results consistently show that with the increase in the epoxy resin temperature, the morphology of the trees changes from branch type to mixed bush-branch type, the fractal dimension of the trees increases, and the breakdown time delay of the specimens is shortened, which is caused by the increase in dielectric constant, the dielectric loss angle tangent value and the phase diffusion coefficient. In addition, the simulation results show that the electrostatic energy distribution of the specimens has a significant effect on the treeing process, and the higher the electrostatic energy is, the faster trees develop. The results of this paper may help to understand the initiation and growth of electrical trees and to optimize insulation materials from an energetic point of view.
Gas switch is one of the key elements in pulsed-power devices, and electrode erosion is a key restrictive factor in high-power gas switch development and application. According to the thermal equilibrium equation near the electrode surface, this paper calculates electrode heat fluxes and their peak powers caused under different discharge conditions, and analyses their effects on the removal method of electrode materials. When discharge current is not too high, calculation results indicate that the arc joule heat is the main cause of electrode erosion and solid material removal may appear. Vaporization of electrode material is the main cause of electrode erosion when discharge current is high enough.
As a critical component of a high-voltage direct current (HVDC) transmission system, resin impregnated paper (RIP) wall bushing has become a weak point because of its surface charge accumulation. This paper studies a model RIP wall bushing core designed by the equal capacitance method. The stationary resistive field along the gas–solid interface of the RIP wall bushing core is investigated theoretically by a gas model, which considers the non-linearly field-dependent volume conductivity. The results show that the gas conductivity along the core surface tends to be an arched distribution from the high-voltage conductor to the end shielding screen. The surface charge mainly accumulates at the turning point of the radius, which may threaten the core’s insulation. Then, the surface charge is obtained through a measurement system, where the experimental results are highly consistent with the simulation results. Considering the time constant of charge dissipation is nearly 15 min, it would be better to measure the surface charge on one axial direction of RIP wall bushing core after each voltage application. The simulation and experimental results of this paper can guide the design of a RIP wall bushing core.