Poly(vinylidene fluoride-hexafluoropropylene) (PVDF-HFP) porous membranes are fabricated via thermally induced phase separation (TIPS) with mixed diluent (dibutyl phthalate (DBP)/dioctyl phthalate (DOP)). The effects of mixed diluent are discussed in detail in term of morphology, mean pore size, selective wettability, etc. The results show that the membrane structure changes from spherulitic to bicontinuous with the change of DBP/DOP ratio. It is also found that the degree of crystallization decreases with the decrease of DBP/DOP ratio in mixed diluent. When liquid–liquid (L-L) phase separation precedes solid–liquid (S-L) phase separation, the obtained membranes have outstanding hydrophobicity and lipophilicity, excellent mechanical property. Additionally, the PVDF-HFP hybrid membranes are prepared with silica (SiO2) particles and the effect of SiO2 content on structure and properties is discussed. It is found that the PVDF-HFP hybrid membrane with 2 wt % SiO2 (M3-S2) has better properties and higher filtration rate and separation efficiency for surfactant-stabilized water-in-oil emulsion separation. Moreover, the membrane M3-S2 also exhibits excellent antifouling performance for long-running.
1 September 2011 in Journal of Materials Chemistry
Poly(tetrafluoroethylene-co-hexafluoropropylene) (FEP) hollow fiber membranes have been fabricated for the first time via the melt spinning method. Dioctyl phthalate (DOP) as the diluent and a composite powder (composed of soluble and insoluble particles) as the pore-creating agent were used in this study. The addition of the composite powder brought about a dissolved pore structure and interfacial microvoids (IFMs) in the membrane. The membrane’s corresponding microfiltration performance was characterized in terms of pure water flux, a mechanical strength test, a mean pore size measurement and morphology observations by a field emission scanning electron microscope (FESEM). The results show that the FEP hollow fiber membrane was a kind of homogeneous membrane, with mean pore sizes ranging from 0.4 to 1 μm. The increase of the composite powder addition and the stretching process brought about an obvious enhancement of the pure water flux and porosity. Compared with the available commercial PTFE hollow tube membranes, the smaller size of the FEP hollow fiber membrane provides a higher filled density in the membrane modules. Moreover, the smaller thickness of the membrane improves membrane permeability.
Novel poly(tetrafluoroethylene) (PTFE) hollow fiber membranes were successfully fabricated by electrospinning, with ultrafine fibrous PTFE membranes as separation layers, while a porous glassfiber braided tube served as the supporting matrix. During this process, PTFE/poly(vinylalcohol) (PVA) ultrafine fibrous membranes were electrospun while covering the porous glassfiber braided tube; then, the nascent PTFE/PVA hollow fiber membrane was obtained. In the following sintering process, the spinning carrier PVA decomposed; meanwhile, the ultrafine fibrous PTFE membrane shrank inward so as to further integrate with the supporting matrix. Therefore, the ultrafine fibrous PTFE membranes had excellent interface bonding strength with the supporting matrix. Moreover, the obtained ultrafine fibrous PTFE hollow fiber membrane exhibited superior performances in terms of strong hydrophobicity (CA > 140°), high porosity (>70%), and sharp pore size distribution. The comprehensive properties indicated that the ultrafine fibrous PTFE hollow fiber membranes could have potentially useful applications in membrane contactors (MC), especially membrane distillation (MD) in harsh water environments.
1 January 2013 in Separation and Purification Technology