This study used the powder metallurgy method to produce particle-reinforced hybrid Al metal matrix composites (HAMMCs). The synergistic effects of adding graphite-TiO2 and ZrO2 reinforcement to the Al matrix on the microstructure development, hardness, and wear behavior of hybrid aluminum metal matrix composites were researched. Hybrid composite samples produced after sintering, phase and microstructure analysis, density measurement, hardness, and wear behavior have been studied experimentally. Microstructural observation shows reinforcements are partially homogeneously distributed in the Al matrix. Dual-oxide reinforcement improved hardness more remarkably than mono-oxide reinforcement in the produced samples. The highest hardness value is obtained in the Al–5% TiO2 + 5% ZrO2 + 2% C composite. The lowest COF values of composite samples are obtained with dual-oxide reinforcement. Al–5% TiO2 + 5% ZrO2 + 2% C composite has the highest wear resistance.
3 June 2026 in Afyon Kocatepe University Journal of Sciences and Engineering
B₄C matrix composites were produced using the spark plasma sintering (SPS) method at a temperature of 1900°C and a pressure of 40 MPa. In the production process, WC additives at volumes of 15%, 17.5%, and 20% and Y₂O₃ additives at volumes of 2.5% and 5% were used. The mechanical properties of composites produced using the SPS method have been investigated in relation to the effect of secondary phases on the structure. The sintered ceramic matrix composites exhibited a high fracture toughness of 8.1 MPa⋅ m¹/² and a Vickers hardness of 23.5 GPa. This remarkable improvement is attributed to the reduction in grain size, the formation of secondary phases, and energy loss mechanisms resulting from fracture along grain boundaries.
1 June 2026 in Russian Journal of Non-Ferrous Metals
The range of applications for metal matrix composite materials is expanding daily due to their outstanding characteristics. Copper matrix metal matrix composites are among the first to come to mind for metal matrix composites (MMCs). The areas of use of copper alloys and copper matrix composites are diverse thanks to their mechanical, electrical, corrosion, and abrasion resistance. With the production of composites with a bimetallic matrix, it is possible to produce twice as successful composites with both ceramic reinforcement and bimetallic matrix reinforcement. This study investigated the microstructural, mechanical, and tribomechanical properties of 10% WC reinforced copper matrix composites with varying Ti element addition. The WC-added copper-titanium matrix composites’ relative densities were higher than 92%. X-ray Diffraction (XRD), Scanning Electron Microscopy (SEM), and Scanning Electron Microscopy with Energy Dispersive X-ray Spectroscopy (SEM-EDS), SEM elemental mapping (SEM-mapping) analyses were performed on the composites, and the phases and grain structures developed during heat treatment were examined. In addition, electrical conductivity measurements showed a significant decrease in the conductivity of WC-doped Cu matrix composites due to the increase in the Ti ratio. Dry sliding wear tests were conducted using a ball-on-disk configuration. The Ti-reinforced Cu matrix composite containing 8% Ti by volume has a hardness of 154.5 HV and wear rate of 4.9 × 10–5 mm3/(N m), exhibiting approximately 1.12 times higher hardness and 12 times greater abrasion resistance compared to the composite without Ti addition. Considering the widespread use of copper matrix composites in sectors such as automotive, aircraft, etc., WC and titanium-doped copper matrix composites are promising thanks to their superior properties.
The powder metallurgy technique is utilized in this study to produce Cu matrix hybrid composites with ZrO2 reinforcements and graphite additives. This study compares composites' microstructural (theoretical, experimental, and relative density, phase morphology, type, chemical content), mechanical (microhardness), and tribological behavior (wear and friction) with 5, 10, and 15 wt% reinforcement, together with and without the effect of 2 wt% graphite additives. Homogenously ZrO2 added copper alloy was successfully produced. All samples were produced at least %90 relative density. The XRD analyses also validate the phase presence of reinforcement phase. Also the graphite was added to samples which provides self-lubrication. The graphite addition improves friction behaviour. The hardness of the composites increased as the amount of ZrO2 increased with the addition of graphite. The wear resistance of ZrO2-added copper samples was improved between 1.32 and 4.84 times better than that of copper without reinforcement.