A new layered heterostructure composite material system (TC4 as front layer and 2024Al alloy as back layer) was developed and analyzed for its design and performance in terms of an enhanced absorption capability and anti-penetration behavior. The Florence model for energy absorption was modified, so that it can be utilized for the layered heterostructure composite material system with more efficacy. Numerical simulation through Ls-Dyna validated the analytical model findings regarding the energy absorption of the system and both were in good agreement. Results showed that two ductile materials with diverse properties, the hardness gradient and varied layer thickness joined together, specifically behaved like a unified structure and exhibited elastic collision after slight bending, which is possibly due to the decreased yield strength of the front layer and increased yield strength of the second layer. To validate the analytical and numerical findings, the samples of the layered heterostructure composite material system were subjected to a SHPB (Split Hopkinson pressure bar) compression test. The deformation behavior was analyzed in the context of the strain energy density and stain rate sensitivity parameter at different strain rates. The encouraging results proposed that two ductile materials with a hardness gradient can be used as an alternate structure instead of a brittle–ductile combination in a layered structure.
17 January 2025 in Journal of Manufacturing Science and Engineering
The hot deformation behavior of AA2024/SiC composite was investigated by experimental and finite element simulation (FEM) methods. The influence of different particle volume fractions and sizes on the mechanical behavior of AA2024/SiC composites was studied. An integrated numerical model was developed using a modified Johnson-Cook model for the AA2024 matrix implemented via VUHARD subroutine and the Johnson-Holmquist model 2 for the SiC particles. Simulations were performed at higher temperatures (673-753 K) and varying strain rates (0.01-1s−1) within random microstructure-based FEM framework using ABAQUS. The FEM results are in close agreement with the experimental data, particularly in the true stress-strain curves, indicating that the developed FEM model effectively captures the hot workability of AA2024/SiC composites under varying temperature conditions, SiC volume fractions, and particle sizes. The results showed that the reinforcement of SiC particles into the AA2024 matrix significantly improved its hot workability by reducing dislocation mobility. The flow stress of composites increased with SiC content and decreased with the reinforcement particle size. The composites reinforced with 5 μm SiC particles had a higher peak flow stress of 145.945 MPa than the others at 673 K and a strain rate of 1s−1. Similarly, at constant temperature and strain rate, the peak flow stress of the composite material increased from 87 MPa to 145.945 MPa (PS = 5 μm, at 673 K and strain rate 1 s−1) as the VF increased from 1% to 20%.
The mechanical properties of music wire are contingent upon its microstructure, which in turn influences its applications in music. Chinese stringed instruments necessitate exacting standards for comprehensive performance indexes, particularly with regard to the strength, resilience, and rigidity of the musical steel wires, which differ from the Western approach to musical wire. In this study, SWP-B music wire was selected for investigation through metal heat treatment, which was employed to regulate its microstructure characteristics. Furthermore, a spectral analysis was conducted to evaluate the musical expression, encompassing attributes such as pitch and timbre. In conclusion, the governing law of the impact of the microstructure of music wire on its musical expression was established. The results demonstrate that steel wire subjected to a 200 °C annealing treatment for cementite spheroidization can effectively reduce stress concentration, thereby reducing the probability of fracture and consequently improving tonal uniformity and richness while increasing tensile strength from 2578 MPa to 2702 MPa. Conversely, the high-temperature annealing treatment alters the crystalline structure of the material and refines the grain structure, thereby improving the material’s performance and sound quality. The fine microstructure of the music steel wire displays enhanced uniformity. As the annealing temperature increases, the strength of the ferrite phase //ND (//ND, indicating that the direction of the crystal is parallel to the normal direction of the material) and the cementite phase //ND demonstrates a gradual decline. However, this also results in a more pronounced harmonic performance, which, in turn, affects the overall music expression.
29 April 2026 in Metals and Materials International