Ti–In–Zn–O (TIZO) and TIZO/Ag/TIZO multilayer transparent films were prepared at room temperature on glass substrates using an RF/DC magnetron sputtering system. The optical and electrical properties of the multilayer structures were examined according to the thickness of each TIZO/Ag/TIZO layer. A transparent and conductive film with a sheet resistance of 11.1 Ω/□ and a transmittance of 86.9% at 550 nm (94.2%, normalized to the glass substrate) was obtained at a TIZO/Ag/TIZO thickness of 100/8/42 nm. The TIZO and TIZO/Ag/TIZO multilayer films exhibited higher mechanical resistances against an increasing load of external scratches than the indium tin oxide (ITO) film. Overall, the properties of the TIZO/Ag/TIZO multilayer films were comparable or superior to those of the ITO/Ag/ITO multilayer. The deposited TIZO/Ag/TIZO multilayer films were used in the fabrication of dye-sensitized solar cells (DSSCs) as the transparent electrode. The TIZO/Ag/TIZO multilayer-based DSSCs exhibited a short circuit photocurrent density of 9.4 mA/cm2, a photocurrent of 613 mV, and an overall cell efficiency of 3.1% at a light intensity of one sun.
Glazes of (70 − x) ZnO-30 B2O3-x Bi2O3 with different Bi2O3 contents were prepared by the conventional melt quench technique. Differential scanning calorimetry (DSC) curves were obtained to determine the glass transition temperature (Tg) and crystallization temperature (Tc) of the glazes. The activation energy of the glass transition (Eg) and crystallization (Ec) were calculated using the Moynihan and Kissinger models, respectively. The glass transition temperature (Tg) decreased linearly with increasing Bi2O3 content. This is because the larger Bi3+ ions reduced network connectivity and opened up the structure. The Tg increased gradually with increasing heating rate (β). This is because the higher heating rate provided more energy for the glass to transition to the liquid state. The activation energy of the glass transition (Eg) decreased with increasing Bi2O3 content. This indicates that the glass-forming ability of the system increased with increasing Bi2O3 content. The energy corresponding to the amorphous-to-crystalline transformation during nucleation and crystal growth (Ec) increased with increasing Bi content to about 30%, and then decreased above 40%. This suggests that higher Ec values have an advantage in preventing crystallization in the crystallization danger region. It can be seen that the addition of Bi2O3 in (70 − x) ZnO-30 B2O3-x Bi2O3 glazes affects the density and distribution of oxygen atoms in the glass structure. It can also be seen that the increased Bi content promotes the formation of Bi-O-Bi bonds, which act as network modifiers to reduce the number of non-cross-linked oxygen atoms and increase network connectivity.
316L stainless steel is widely employed in various industrial sectors, including shipbuilding, offshore plants, high-temperature/high-pressure (HTHP) piping systems, and hydrogen infrastructure, due to its excellent mechanical stability, superior corrosion resistance, and robust resistance to hydrogen embrittlement. This study presents 316L stainless steel alloys fabricated via hot isostatic pressing (HIP), conducted at 1300 °C and 100 MPa for 2 h, incorporating Cr2N powder and an optimized Ni/Mn ratio based on the nickel equivalent (Ni_eq). During HIP, Cr2N decomposition yielded a uniformly refined, dense austenitic microstructure, with enhanced corrosion resistance and mechanical performance. Corrosion resistance was evaluated by potentiodynamic polarization in 3.5 wt.% NaCl after 1 h of OCP stabilization, using a scan range of −0.25 V to +1.5 V (Ag/AgCl) at 1 mV/s. Optimization of the Ni/Mn ratio effectively improved the pitting corrosion resistance and mechanical strength. It is cost-effective to partially substitute Ni with Mn. Of the various alloys, C13Ni-N exhibited significantly enhanced hardness (~30% increase from 158.3 to 206.2 HV) attributable to nitrogen-induced solid solution strengthening. E11Ni-HM exhibited the highest pitting corrosion resistance given the superior PREN value (31.36). In summary, the incorporation of Cr2N and adjustment of the Ni/Mn ratio effectively improved the performance of 316L stainless steel alloys. Notably, alloy E11Ni-HM demonstrated a low corrosion current density of 0.131 μA/cm2, indicating superior corrosion resistance. These findings offer valuable insights for developing cost-efficient, mechanically robust corrosion-resistant materials for hydrogen-related applications. Further research will evaluate alloy resistance to hydrogen embrittlement and investigate long-term material stability.
Superplastic deformation, which occurs when fine-grained metals exhibit high ductility (often exceeding 300%) under specific conditions at approximately half of their melting temperature, allows the creation of complex shapes required by the aerospace and electronic material industries. Typically, superplastic characteristics are evaluated using universal testing machines (UTMs). However, nickel (Ni) and its alloys, which are applied as electrodeposits in the fabrication of electronic materials, are nanocrystalline in nature and exhibit superplasticity under specific temperatures and deformation conditions. Electrodeposited foils are very thin, making traditional UTM testing challenging; therefore, a new approach is required. In this study, we used a thermomechanical analyzer (TMA) to analyze the superplastic properties of electrodeposited nickel foils simply and precisely. TMAs are particularly appropriate when evaluating thin foils because they yield detailed thermal deformation data, whereas UTMs do not. A TMA reveals thermal deformation of electrodeposited nickel foils across various temperatures, as well as microstructures and grain growth. We performed superplastic analysis at 400 °C, 500 °C, and 600 °C at a strain rate of 1 × 10−3 s−1, and microstructural data were obtained through X-ray diffraction and electron backscatter diffraction. Superplastic deformation was apparent at 400 °C. The data obtained through our systematic analysis using a TMA will guide future studies on the application of superplastic properties of electrodeposited nanocrystalline nickel foils.