To improve the hearth activity and provide a theoretical basis for the blast furnace (BF) smooth operation, this paper introduced indirect indicators of hearth activity, such as the descent of burden, fluctuations in air volume and pressure, hearth temperature, iron tapping conditions, and the heat of slag iron. The factors influencing hearth activity were analyzed, primarily focusing on the permeability provided by deadman, the viscosity of slag iron, and the position and size of the tuyere raceway. Control measures for hearth activity were summarized, including adjusting the permeability provided by deadman by controlling the particle size distribution and strength of coke. Maintaining the appropriate viscosity of slag iron by controlling the temperature of slag iron, the binary alkalinity of slag, the magnesia-to-alumina ratio, and the elemental content of sulfur, silicon, manganese, and titanium in the iron. Adjusting the position of the tuyere raceway by controlling parameters such as air volume, air pressure, tuyere area, and oxygen enrichment rate. Finally, it was concluded that providing more permeability channels through deadman, maintaining the viscosity of slag iron within a suitable range, and promoting the development of the tuyere raceway towards the lower and central parts of the furnace are all beneficial for improving hearth activity.
The molecular dynamics simulation technique was utilized to examine the structural variations of the Cu95Fe5 alloy, as well as the precipitation and aggregation processes of Fe atoms during heat preservation. It is shown that the crystallization temperature of the Cu95Fe5 alloy under the condition of a 2 × 1010 K/s cooling rate is 882 K. Crystallization of the alloy occurs when it is insulated under the temperature conditions of 900 K, 1000 K, and 1100 K. The lower the holding temperature, the shorter the holding time required for the system to initiate crystallization. In other words, lower temperature holding facilitates easier crystallization. The formation process of Fe clusters has been investigated. The size and quantity of Fe clusters at various stages are influenced by the interatomic interaction forces between Fe atoms, the diffusion capabilities of Fe atoms, the local structural rearrangement of nondispersive atoms, and the interfacial energy between Fe clusters and the Cu matrix. The formation of Fe clusters in the insulation process mainly undergoes four stages: First, the initial small clusters are disassembled under the influence of molecular thermal motion and the attractive interactions between Fe atoms. This process leads to the formation and growth of new small clusters. Secondly, the clusters condense and grow under non-diffusive atomic local structure rearrangement. Third, the Fe clusters are sphericalized under Cu-Fe interfacial energy. Fourth, individual Fe atoms are diffused into large Fe clusters under the action of molecular thermal motion.