A flame-retardant treatment for cellulosic paper was applied by spraying the paper with combinations of lignin, phytic acid, and sodium silicate. Lignin enhanced the flame retardancy in the condensed phase, while phytic acid provided dual-phase flame resistance. Sodium silicate further improved thermal stability by forming silica gel through its reaction with phytic acid. The limiting oxygen index increased from 16.8% to 22.0%, and in vertical flame tests, treated paper self-extinguished within 1.5 s, whereas untreated paper burned completely in 12.0 s. Thermogravimetric analysis revealed enhanced thermal stability, with treated paper retaining 36.5% residual char at 900 °C compared to 0% in untreated paper. Despite the relatively low coating coverage from the spray deposition method, the synergistic interaction of phytic acid, lignin, and silica gel effectively compensated by promoting dense char formation and thermal insulation. Fire retardancy was attributed to phytic acid-catalyzed lignin and silica composite formation in the char layer, enhancing structural stability and shielding efficiency. Raman spectroscopy confirmed improved graphitization (ID/IG = 1.20), while scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM-EDX) and Fourier transform infrared spectroscopy (FT-IR) verified phosphorus and silica retention. This treatment showed potential for high-performance flame-retardant cellulose materials in packaging, construction, and other industries.
30 June 2025 in Journal of Korea Technical Association of The Pulp and Paper Industry
Considering the continuous demand for environmentally friendly materials in modern industrial and environmental fields, the paper industry, which is a leading sector in cellulose utilization, is focusing substantial efforts on the development of sustainable materials and expansion of its market presence. Increasing attention is being directed toward functional packaging materials that can replace plastics and a wide range of advanced functional
A reinforced composite aerogel composed of carboxymethyl chitosan (CMCS) and cellulose nanofibers (CNFs) was synthesized via chemical crosslinking with epichlorohydrin (EH) for the efficient removal of Pb(II) ions from aqueous solutions. The CMCS, a chitosan derivative, was successfully prepared through a simple chemical reaction with a degree of substitution of 1.96. The incorporation of CNFs imparted enhanced mechanical stability to the aerogel matrix and increased the surface area, whereas carboxymethyl cellulose contributed functional carboxyl groups that facilitated efficient metal ion adsorption. In addition, crosslinking with EH significantly improved the structural integrity and water stability of the aerogels, rendering them suitable for application in aqueous environments. The composite aerogels exhibited a porous structure and good adsorption of lead ions (Pb2+) in water with a removal percentage of 98%. Upon the addition of 1 wt% CNF loading, the compression strength of the composite aerogels was enhanced 42% compared with the samples without CNF loading. The adsorption kinetics showed a high correlation with the pseudo-second-order model (R² = 0.99). The good structural stability and water absorption of the prepared CMCS aerogels make them an ideal candidate for eco-friendly heavy metal-ion treatment.
In recent decades, lignocellulosic biomass has attracted increasing attention as a sustainable alternative to fossil-fuel-based resources. However, the compact and highly crystalline structure of cellulose remains a major limitation to its effective utilization. In this study, the allomorphic transformation of cellulose was induced through chemical treatments using sodium hydroxide (NaOH) and ethylenediamine (EDA), enabling the conversion of native cellulose I into cellulose II and cellulose III, respectively. The resulting changes in the crystalline structure were systematically investigated using X-ray diffraction and Raman spectroscopy. Both NaOH- and EDA-treated celluloses exhibited enhanced enzymatic digestibility compared to untreated cellulose, consistent with the observed modifications in the crystal structure. Nevertheless, some results indicate that crystalline structure is not an absolute determining factor, but rather one of several parameters, including specific surface area, particle size, and degree of polymerization.
This study investigates the surface characteristics of printing papers using fractal geometry, focusing on surface roughness and surface friction as independent properties. The fractal dimension (FD) was analyzed using the power spectral density method, which provided a more distinct characterization of paper surfaces compared to the variogram method. Surface roughness and friction were measured using a stylus-based contact profilometer, and mean absolute deviation (MAD) parameters, such as the mean absolute deviation of surface roughness (RMAD) and friction, were calculated to capture surface variability. The results revealed that while conventional parameters, such as roughness average (Ra) and the average coefficient of friction, are highly sensitive to measurement conditions, MAD-based parameters demonstrate greater robustness and stability. For instance, the regression equation for RMAD vs. Ra showed a strong correlation, with an R² value close to 1.0. However, the slopes were significantly less than one. Furthermore, FD exhibited weak correlations with surface roughness and friction, with R² values of 0.342 and 0.016, respectively, highlighting its unique ability to characterize autocorrelation or complexity of surface. Additionally, the effects of coating on paper surfaces were evaluated, revealing reduced flocculation of surface profiles but a 5% increase in FD, indicating enhanced surface complexity. These findings underscore the complementary role of FD in providing a comprehensive understanding of surface properties, with potential applications in quality control and the design of paper products.