20 January 2022 in ACS Omega
Verified
Journal Article
Open access
HLHui Li
Hui Li
zhihang lizhihang li
zhihang li
JJJianping Jin
Jianping Jin
YHYuexin Han
Yuexin Han
YLYanjun Li
Yanjun Li
Refractory gold ore is usually affected by the associated carbonaceous matter through the preg-robbing effect, which is eliminated by oxidation roasting, followed by leaching, to achieve a satisfactory gold leaching efficiency. Roasting–leaching experiments, pore structure measurements, scanning electron microscopy (SEM), and X-ray diffraction are used to explore the structural evolution of pores on the surface and its effect on the leaching performance. Pores with optimal sizes were obtained by roasting at 650 °C for 2.0 h with a ventilation of 0.6 m3/h; approximately 92.55% gold could be recovered under these conditions. A porous structure observed by SEM became more compact as the temperature further increased to 850 °C. The formation of CaSiO3 and CaSO4 in pores led to pore shrinkage. The mechanism of oxidation roasting, followed by cyanide leaching, was schematically analyzed and revealed the effects of pore structural evolution and phase transformation on the leaching efficiency.

26 February 2021 in Minerals
Verified
Journal Article
Open access
PDF file
JJJianping Jin
Jianping Jin
ZWZhou Wentao
Zhou Wentao
YSYongsheng Sun
Yongsheng Sun
YHYuexin Han
Yuexin Han
YLYanjun Li
Yanjun Li
It is particularly significant to investigate the reduction behavior and existing form of phosphorus in metal and slag phase during coal-based reduction for the efficient development and utilization of high-phosphorus oolitic hematite. The reduction behavior of phosphorus minerals and their existing form in the metal and slag phase during the coal-based reduction of high phosphorus oolitic hematite were systematically investigated using HSC software simulation, thermodynamic calculation, X-ray diffraction (XRD), scanning electron microscopy (SEM), and energy-dispersive spectrometry (EDS). The results show that after Fe2O3 was reduced to metal iron, the reduction of apatite was promoted by providing the most inclined enrichment site of phosphorus (metallographic phase). Phosphorus existed mainly in two forms in the metal phase—one was in the form of Fe3P compound at the boundary of the metal phase, and the other was in the form of solid solution in the metal iron. There were two forms of phosphorus in the slag phase—one was incompletely reacted apatite, and the other was formed as CaO–SiO2–P2O5 solid solution. In the early stage of coal-based reduction, phosphorus in the slag phase mainly existed in the form of apatite, while in the later stage, it mainly existed in the form of CaO–SiO2–P2O5 solid solution.