Cyclosporin A (CyA) is a good candidate for incorporation in colloidal carriers such as nanoparticles (NP) that would diminish the adverse effects associated with its use under conventional pharmaceutical dosage forms and improve bioavailability after oral administration. In this study a composite rotational experimental design was used to evaluate the joint influence of five formulation variables: temperature of the aqueous phase, needle gauge, volume of the organic phase, and the amounts of polymer and surfactant on the micromeritic characteristics of the CyA-loaded NP obtained by the method of Fessi et al. The percentage of drug encapsulated in the NP was also evaluated for each formulation, and the yield, which was expressed as the ratio between the experimentally measured quantity of drug in the formulation and the theoretical content, was determined because CyA undergoes surface absorption. Potential variables such as stirring speed (500 rpm), final drug concentration (100 micrograms/mL), or injection rates (GRi = 0.379 mL/s) were maintained constant. The ANOVA corresponding to the experimental design showed that the amounts of polymer and surfactant, and the diameter of the needle used in the preparation of NP, significantly affected the percentage of entrapped drug (I2 = 0.8916). The mean particle size was significantly affected by all the formulation variables tested except for the amount of surfactant dissolved in the external aqueous phase (r2 = 0.9518). Neither the yield (mean value of 99.61%) nor the size distribution parameters (polydispersity and coefficient of variation) presented good correlation coefficients for the equations obtained, although some variables showed statistical significance. A second study was carried out to investigate the effects on the drug-loaded NP characteristics of varying the global injection rates (GRi) for the organic phase into the aqueous medium. The results showed a dramatic decrease in both particle size and drug incorporation in the carrier as the rate of mixing increased. From the results of both the experimental design and the second study, a theoretical model for nanoparticle formation is proposed that considers the most significant variables, and an empirical relationship to predict mean particle size is presented. Thus, particle size can be controlled by the injection rates (GRi), the needle gauge, and the polymer concentration.
1 January 2017 in International Journal of Pharmaceutics
Purpose: Dry eye (DE) includes a group of diseases related to tear film disorders. Current trends for DE therapy focus on providing lipid components to replace the damaged lipid layer. Formulations that contain aqueous and mucin-like compounds may have additional therapeutic benefits for DE patients. The aim of this work was to design and evaluate novel formulations having the potential to become topical treatment for DE. Methods: Unpreserved liposomal formulations composed of phosphatidylcholine (PC), cholesterol, and α-tocopherol (vit E) were prepared by the thin-film hydration technique. Formulations were characterized in terms of liposome size, pH, surface tension, osmolarity, and viscosity. In vitro tolerance assays were performed on macrophage, human corneal and conjunctival cell lines at short and long term exposures. In vivo ocular tolerance was studied after instillation of the formulation. Results: The mean liposome size was less than 1 µm and surface tension <30 mN/m for all formulations. The final liposomal formulation (PC:cholesterol:vit E in a ratio 8:1:0.8) had physiological values of pH (6.45 ± 0.09), osmolarity (289.43 ± 3.28 mOsm), and viscosity (1.82 ± 0.02 mPa∙s). Cell viability was greater than 80% in the corneal and conjunctival cells. This formulation was well tolerated by experimental animals. Conclusions: The unpreserved liposomal formulation has suitable properties to be administered by topical ophthalmic route. The liposome-based artificial tear had good in vitro and in vivo tolerance responses. This formulation composed of a combination of liposomes and bioadhesive polymers may be employed successfully as a tear film substitute in DE therapy.