Additive manufacturing (AM) has the potential to produce novel high-performance electrical machines, enabling the direct printing of complex shapes and the simultaneous processing of multiple feedstocks in a single build. We examined the properties and functional performance of Fe-3 wt.% Si materials that were printed via selective laser melting, machined down to thin laminates, and stacked to form a stator core of a prototype brushless permanent-magnet electrical motor. Big Area Additive Manufacturing of Nd2Fe14B (NdFeB)–polyphenylene sulfide (PPS) bonded magnets was performed, with them then being magnetized and used for the rotor. The magnetic, mechanical, and electrical properties of the as-printed and various heat-treated thin laminates and the back electromotive force (EMF) of the electrical motors at different rotational speeds were measured. The thin laminates exhibit a maximum relative permeability of 7494 at an applied field of 0.8 Oe and a core loss of about 20 W/lb at 60 Hz with the maximum induction of 15 kg. In addition to the demonstration of AM printing, motor assembly, and complete characterization of printed Fe-3 wt.% Si, this report highlights the areas of improvement needed in printing technologies to achieve AM built electrical motors and the need for isotropic microstructure refinements to make the laminates appropriate for high-mechanical-strength and low-loss rotational electrical devices.
Research into the processability of NiTiHf high-temperature shape memory alloys (HTSMAs) via laser powder bed fusion (LPBF) is limited; nevertheless, these alloys show promise for applications in extreme environments. This study aims to address this limitation by investigating the printability of four NiTiHf alloys with varying Hf content (1, 2, 15, and 20 at. %) to assess their suitability for LPBF applications. Solidification cracking is one of the main limiting factors in LPBF processes, which occurs during the final stage of solidification. To investigate the effect of alloy composition on printability, this study focuses on this defect via a combination of computational modeling and experimental validation. To this end, solidification cracking susceptibility is calculated as Kou’s index and Scheil–Gulliver model, implemented in Thermo-Calc/2022a software. An innovative powder-free experimental method through laser remelting was conducted on bare NiTiHf ingots to validate the parameter impacts of the LPBF process. The result is the processability window with no cracking likelihood under diverse LPBF conditions, including laser power and scan speed. This comprehensive investigation enhances our understanding of the processability challenges and opportunities for NiTiHf HTSMAs in advanced engineering applications.