Silicon carbide (SiC) nanorods were synthesised by reacting multi-walled carbon nanotubes (CNTs) with Si particles in a NaCl–NaF binary salt for 4 h at 1100–1200 °C in Ar. Reaction products were analysed by a combination of X-ray diffraction (XRD) and transmission electron microscopy (TEM), including aberration corrected lattice imaging and electron energy loss spectroscopy (EELS). At 1100 °C, 3C–SiC became detectable by XRD but unreacted Si and CNTs were still dominant, while, at 1150 °C, SiC increased at the expense of Si and CNTs. Finally, at 1200 °C, only SiC peaks were seen, indicating the complete conversion from CNTs to SiC nanorods. This synthesis temperature is 200–250 °C lower than that required by the conventional vapour–solid reaction process. The resultant SiC nanorods mostly followed the morphologies of the as-received CNTs, indicating that CNTs had not only served as carbon source but also acted as the templates for the nanorod growth. Most of the resultant SiC nanorods had complex stacking sequences containing various forms of stacking faults, and only some exhibited regular fault-free stacking sequences.
α-Si3N4 nanobelts were grown on a graphitic carbon felt via an improved Ni-catalyzed chemical vapor deposition (CVD) process. The as-prepared nanobelts were up to several millimeters long and 300–1200 nm wide exhibiting a unimodal diameter distribution with peak range at 500–600 nm. Ni originally mixed with Si partially evaporated and then condensed on the carbon felt surface, forming catalytically active centers which absorbed gaseous Si and N and accelerated the growth of α-Si3N4 nanobelts. The formation process is considered to be co-dominated by a vapour–liquid–solid (VLS) base-growth mechanism and a vapour–solid (VS) tip-growth mechanism. The former was responsible for the initial nucleation and the proto-nanobelt formation and successive base-growth along the [101] direction of α-Si3N4, and the latter additionally contributed the growth at tips. The formation of α-Si3N4 nanobelts instead of nanowires is attributed to the anisotropic growth in the width and thickness directions, dictated by the liquid Ni catalyst droplets, in particular, in the initial proto-nanobelt formation stage. The room-temperature photoluminescence spectrum showed that the as-synthesized α-Si3N4 nanobelts had a strong emission with two maximum peaks at 416 nm (2.98 eV) and 436 nm (2.84 eV) located in the violet-blue spectral range, making it a potential material for applications in LED and optoelectronic nanodevices.
20 May 2010 in International Journal of Applied Ceramic Technology