The present study is aimed at investigating Mechanical properties of the milled recycling Aluminium type AA6061 according to the change of the volume fraction for the continents and the reinforcement material. In the study, high speed millings were used for producing the chip sizes of AA6061 and followed by a cold press forging process. Milling process was used to produce smaller particles of aluminium chips by the planetary ball mill. Three groups of specimens were taken according to the percentage of chip and powder, while, two groups were taken according to the mixture between different particle sizes of powders. Where, four types of particle size were chosen (25, 63, 100, mix of particles) μm. The results were showing that the Microhardness increased with increasing the percentage of chip, then the density was decreased due to a large amount of pores were found. By the experiments, it can be concluded, the mixture of powders is the best choice for all groups. On the other hand, the type D3 (78.5% (25μm) + 21.5% (100μm)) gave the best result for microhardness compare with others according to particle.
1 January 2019 in Journal of Physics: Conference Series
Microhardness and microstructure become a main concern in direct recycling of metal chips. Products by solid-state recycling of aluminum chips in hot extrusion process are controlled by many factors such as die geometry, extrusion ratio, temperature related parameters and etc. in which each of them could influence the extrudate's quality. This study investigates the effects of preheating temperature and preheating time on the response variable (microhardness and microstructure). The various settings of preheating temperature were taken as 450 °C, 500 °C, and 550 °C. On the other hand, three values of preheating time were chosen (1, 2, 3) hours. The influences of the process parameters (preheating temperature and time) were analyzed using Design of Experiments (DOE) approach whereby full factorial design with center point analysis was adopted. The total runs were 11 and they comprise of two factors of full factorial design with 3 center points. The results found that the preheating temperature is more important to be controlled rather than the preheating time in analysis of microhardness and decreasing of temperature led to the high microhardness. The profile extruded at 450 °C and 1 hr had gained the optimum microhardness and it can be concluded that setting temperature at 550 °C for 3 hour resulted in the highest responses for average of grain sizes in analysis of microstructure.
Solid-state recycling is a sustainable technique for recycling aluminium scrap, and the process before recycling is essential to control the physical properties of the product. In this work, the effect of the thermally-treated chips on the extrudate density was investigated. The aluminium chips were thermally-treated to enrich the alumina layer and reduce compaction pressure during chips compaction before recycled using direct hot extrusion. The chips that were transformed into compacted billets were extruded directly without melting and conducted according to 24 full factorial experimental design. The density test on the recycle extrudate found that the density variation ranged from 2724 to 2983 kg/m3. The ANOVA result showed that all factors investigated were statistically significant. The most significant factor was the preheating temperature, followed by extrusion ratio, chip treatment temperature, chip treatment time, and the interaction of chip treatment-time–extrusion ratio. The predictive model suggested by the ANOVA is useful to predict the density with 1% error. Microstructure examination revealed the presence of alumina entrapped in the recycle extrudate, in which thermal-treated chips contained more alumina than that of the untreated chips. The result indicated that the thermal treatment performed on the chips had enriched the in-situ alumina, affecting the density of the recycle extrudate.
Solid state recycling methods allow the production of high density aluminium alloy parts directly from aluminium scrap. Direct conversion approach of recycling of aluminium is relatively easy, less energy usage and environmental friendly. In this paper, AA6061 chips were recycled to fabricate SiC particle (2.5, 5 and 7.5 wt.%) and Al powder (10, 30 and 50 wt.%) reinforced AA6061 alloy matrix composites by the combination cold pressing techniques and sintering process. The effects of various composition of Al and SiC powder on the microstructure of the recycled AA6061/Al-SiC composites showed that the Al and SiC powders in samples were distributed non-homogeneously and randomly between the AA6061 chip regions. The density of sample AA6061/10Al powder gave the closest value to theoretical at 2.43 g/cm3 and decreases when more Al powder were added. The AA6061/10Al-7.5SiC sample showed the highest hardness at 61.0 Hv.
1 December 2018 in International Journal of Integrated Engineering