Nano-size structures, nanotubes/multi-layer graphene (CNT/MLG), were dispersed into epoxy system by a combination of sonication and high shear mixing. To avoid CNT/MLG agglomeration, a non-covalent functionalization were performed using surfactants, CO890 - Polyoxyethylene (40) nonylphenyl ether and SDBS - sodium dodecyl benzene sulfonate. Raman spectroscopy and Fourier transformed Infra-red analysis indicated that CO890-MLG and SDBS-CNT have strong chemical interactions. Atomic force microscopy revealed formation of "spike-like" nanostructures for SDBS-CNT combination and "wall-like" nano-shape structures for the CO890-MLG ones. Tensile tests data indicate no significant change on stiffness. In average, the ultimate stress increased around 18%, while toughness had an improvement close to 62%. SDBS-CNT and CO890-MLG at small concentrations (0.075 wt. %) are probably the best options for nano-reinforcement of carbon/epoxy composites.
21 September 2022 in International Journal of Adhesion and Adhesives
Carbon nanotubes were employed as adhesive reinforcement/nano-stitches to aluminum bonded joints. The CNT addition to an epoxy adhesive not only lead to an increase on load capacity but it is also the most probable cause of the mixed failure mode (adhesive/cohesive). The damage evolution was described as the stiffness decrease and the failure mixed modes were related to the load capacity. Although the presence of CNT cluster were observed, in small concentrations (< 1.0 wt. %), these clusters acted as crack stoppers and lead to an increase on lap joint shear strength. The addition of 2.0 wt. % carbon nanotubes lead to an increase on load capacity of approximately 116.2 % when the results were compared against the single lap joints without carbon nanotubes.
1 January 2010 in Revista Brasileira de Ortopedia (English Edition)
To investigate the effect of using wrist immobilization orthoses made from different materials, on activation of the flexor and extensor musculature of the forearm while performing specific tasks. Twenty-six adults, with an average age of 26.2 years, underwent the Jebsen-Taylor functional hand test and the grip strength test (Jamar(®) dynamometer) under three conditions: free hand, wearing a composite orthosis and wearing a thermoplastic orthosis. The tests were carried out using the dominant hand only. During the tests, surface electrodes were attached to the flexor and extensor muscles of the forearm to record the muscle electrical activity. The results obtained under the three conditions were compared and analyzed using the Wilcoxon statistical test. Significant differences in muscle activation were found between using the free hand and using any of the orthoses. There was no significant difference in muscle activation between the two types of orthosis. A decrease in activity of the extensor muscles of the forearm was observed during all the tasks, as well as an increase in activation of the flexor muscles with the use of the orthoses. These results are important for defining whether an orthosis should be prescribed during the rehabilitation process for a wide range of disorders, such as tendinitis of the flexors and extensors of the wrist and fingers, as well as for predicting the length of time for which these devices should be used.
Neste estudo, investigou-se a síntese de nanomembranas por eletrofiação (electrospinning). A poliamida-66 (PA-66) foi usada para estudar a influência dos parâmetros operacionais (concentração do polímero, diferença de potencial elétrico aplicada, vazão da solução, distância entre ponta da agulha e o coletor) na morfologia das nanofibras. Também foi estudado o efeito da adição de nanofolhas de grafeno na morfologia das nanofibras. Os resultados demonstraram que o diâmetro médio das nanofibras é diretamente proporcional à vazão, à concentração do polímero e à diferença de potencial elétrico aplicada. A adição de nanopartículas de base carbono fez com que o diâmetro médio das nanofibras aumentasse. Os diâmetros médios para as concentrações de grafeno de 0%, 1%, e 2% variaram de 57 nm (0%) até 141 nm (2%). No entanto, é importante salientar que os diâmetros médios das nanofibras obtidas estão 37% menores que aqueles reportados na literatura.
20 June 2023 in Journal of Vibration Engineering & Technologies