Asphalt mortar plays an important role in the performance of asphalt mixtures. Up to now, there have been many studies on the properties of asphalt mortar. However, asphalt mortar requires a balanced design that considers the overall performance including self-healing capability. Therefore, this study aims to analyze the effect of different types of filler with varied ratios (0.11, 0.22, 0.33, 0.44, and 0.55) by volume on the performance of the asphalt mortar and mixture. The examined fillers were limestone, fly ash, diatomite, and four types of red mud, which were mixed with bitumen to prepare asphalt mortar. Then, the rheological properties of the asphalt mortar were investigated through viscosity tests and multiple stress creep recovery (MSCR) testing. In addition, this research explores the impact of filler type and its ratio on the cohesion and self-healing performance in dry and water conditions. Furthermore, the Hamburg wheel tracking test (HWTT) was performed to evaluate the moisture-damage and rutting resistance of asphalt mixtures, which consisted of the same selected mortar. The results indicate that pull-off tensile strength after the first failure-healing (F-H) cycle in the water condition has a good linear relationship with the dynamic stability of the asphalt mixture in the HWTT. Moreover, red mud and diatomite can be applied as promising substitute fillers compared with the other examined fillers in this study, but the chemical components need to be carefully selected.
The durability of permeable pavement needs to be further studied by accelerated pavement testing (APT). Full-scale APT facilities are commonly associated with a very high initial investment and operational costs. A piece of small-scale accelerated testing equipment, the model mobile load simulator (MMLS), was used to investigate and evaluate the mechanical properties of three types of permeable asphalt pavements, including a 4 cm porous asphalt layer with cement-treated permeable base (4PA-CTPB), 7 cm porous asphalt layer with cement-treated permeable base (7PA-CTPB), and 7 cm porous asphalt layer with cement-treated base (7PA-CTB). Under different conditions of subgrade soil, transverse and longitudinal strains at the bottom of the porous asphalt layer and average rut depth and temperature data were collected. The results indicated that 4PA-CTPB produced the maximum average rut depth but minimum resilient tensile strain. The transverse resilient tensile strain of 7PA-CTPB was significantly higher than the other two structures under both wet and dry conditions. The transverse resilient tensile strain significantly increased with increasing loading cycles with a decreasing rate, which could be affected by both load and temperature. MMLS could be used to explore and evaluate the mechanical properties of permeable asphalt pavement. From the data under dry and wet conditions, it may be better to increase the strength of the subgrade, where a suitable hydraulic conductivity coefficient should be considered.