Constructing efficient conductive networks in flexible polymer matrices remains a central challenge in electromagnetic interference (EMI) shielding material design. In this work, a ‘point-line’ hybrid filler system combining conductive carbon black (CB) and multi-walled carbon nanotubes (MWCNTs) was incorporated into a silicone rubber matrix to systematically engineer the conductive network architecture. By optimising the CB/MWCNT blending ratio, a composite with a tensile strength of 8.5 MPa, elongation at break of 180%, and EMI shielding effectiveness of 50 dB was achieved at a 1:1 weight ratio. Further surface modification of the hybrid fillers using five surfactants, including sodium dodecylbenzene sulfonate (SDBS), cetyltrimethylammonium bromide (CTAB), polyvinylpyrrolidone (PVP), nonylphenol ethoxylate (NPEO), and octylphenol ethoxylate (OPEO), was systematically investigated. OPEO modification was proved the most effective, improving EMI shielding performance to 58 dB while enhancing tensile strength by 11.8% and elongation at break by 50%. These results demonstrate that rational filler hybridisation combined with targeted surfactant modification offers a practical and scalable route to high-performance flexible EMI shielding composites.
Nanocomposites of single-wall carbon nanotubes in isobutylene isoprene rubber (IIR/SWCNTs) were successfully prepared by a simple and green wet process. The traditional melt mixing process and organic solvent dissolution suffered from unable to effectively disperse the SWCNTs of tangled structure, and degradation of polymer molecules, respectively. Our process very well avoided these two problems. The SWCNTs aqueous solutions emulsified by polyoxyethylene octyl phenol ether (OP-10) were firstly mixed and compounded with IIR rubber at a relatively high temperature, followed by the second step of melt compounding process with the addition of cross-linking agent and accelerators. The SWCNTs were dispersed uniformly, and a fine network was constructed in the matrix of the obtained IIR/SWCNTs nanocomposite with a low percolation threshold. With the concentration of SWCNTs as low as 2 phr, the IIR/SWCNTs nanocomposite received an electrical conductivity of 10(-6)similar to 10(-3) S/cm, and a 71% improvement of tensile strength. By varying the loadings of SWCNTs in a certain range, the tensile strength, electrical conductivity, and dielectric property were found tunable. Besides, the nanocomposites also presented strain responsive specific resistance, excellent elongation (600-740%), and better heat resistance.