Here, we propose an optical bistable device structure with a few layers of graphene oxide integrated in the metal-dielectric-metal based asymmetric nanocavity. Through the light confinement in the nanocavity, the third order nonlinear absorption of graphene oxide can be significantly enhanced, which experimentally delivers low-threshold optical bistability at the visible wavelength of 532 nm with only 267 KW/cm2 intensity. In addition, the switching threshold can be further reduced via increasing the graphene oxide thickness, hence paving a new way for achieving tunable optical bistable devices at visible light frequencies.
Perovskite quantum dots (PQDs), with their excellent optical properties, have become a leading semiconductor material in the field of optoelectronics. However, to date, it has been a challenge to achieve the three-dimensional high-resolution patterning of perovskite quantum dots. In this paper, an in situ femtosecond laser-direct-writing technology was demonstrated for three-dimensional high-resolution patterned CsPbBr3 PQDs using a two-photon photoresist nanocomposite doped with the CsPbBr3 perovskite precursor. By adjusting the laser processing parameters, the minimum line width of the PQDs material was confirmed to be 98.6 nm, achieving a sub-100 nm PQDs nanowire for the first time. In addition, the fluorescence intensity of the laser-processed PQDs can be regulated by the laser power. Our findings provide a new technology for fabricating high-resolution display devices based on laser-direct-writing CsPbBr3 PQDs materials.
In this paper, ultra-fast laser lift-off (LLO) of carbon nanotube (CNT)-integrated polyimide film (PI) was investigated by different laser burst mode and pulse intervals using the two-temperature model. By comparing the temperature field distributions of nanosecond, picosecond, and femtosecond lasers at different pulse intervals, it can be found that picosecond lasers cause a higher lattice temperature increase at the PI interface with specific pulse interval conditions. With the increase in the pulse interval, the lattice temperature of the three kinds of lasers decreased, indicating that the heat accumulation effect was weakened. In addition, under picosecond laser irradiation, the lattice temperature at the PI/glass interface of integrated CNTs could be significantly increased, which was significantly different from the system without integrated CNTs. The simulation results show that the picosecond laser is more suitable for LLO with an appropriate pulse interval, and the integration of CNTs at the PI/glass interface can effectively reduce the laser energy threshold required for the LLO process. Our work presents a new PI/CNT/glass model for ultra-fast laser low-threshold LLO and promotes the laser debonding technology in the fields of OLED and other optoelectronic chips.
Laser lift-off (LLO) is a critical process for separating ultra-thin polyimide (PI) films in flexible electronics manufacturing, yet traditional methods often induce thermal and mechanical damage due to high laser energy processing. To address this, we propose a low-threshold LLO method by integrating carbon nanotubes (CNTs) at the interface between a 500 nm PI film and a glass substrate. The interfacial thermal dynamics and separation quality were evaluated through finite element simulations and experimental validations using a 355 nm ultraviolet nanosecond laser. Results demonstrate that CNTs significantly enhance interfacial ultraviolet absorption and promote lateral heat diffusion due to their high axial thermal conductivity. This mechanism broadens the thermal decomposition zone and suppresses vertical heat transfer, thereby reducing the required LLO threshold from 180 mJ/cm2 to 120 mJ/cm2. Furthermore, the integration of CNTs reduces interfacial adhesion and alters the separation dynamics, resulting in the formation of smoother blisters with increased diameters and reduced heights compared to conventional LLO. These effects effectively minimize thermal and mechanical damage to the ultra-thin PI film and its integrated devices. This CNT-assisted LLO approach provides an efficient, low-damage solution for ultra-thin film separation, showing strong potential for advancing high-performance flexible electronics.