With increasing service life, concrete durability gradually deteriorates, requiring urgent repair and reinforcement. Conventional cement-based repair materials exhibit disadvantages such as high brittleness, low tensile strength, poor adhesion, and insufficient durability, making them inadequate for high-quality structural repairs. Based on the molecular structure–activity relationship, this study developed a novel waterborne epoxy–cement-based composite repair material using self-synthesized waterborne epoxy resin (WEP). The mechanism by which WEP improves the performance of cement-based materials was elucidated. The results indicate that WEP significantly influenced the early formation of silicate crystals. Furthermore, the addition of WEP enhanced material flexibility and adhesion, achieving flexural strength of 12.9 MPa and direct tensile bond strength of 2.13 MPa at 28 days, representing increases of approximately 30% and 58%, respectively, compared to the control group. Stress–strain curve analysis revealed that the ultimate strain of WEP-modified cement mortar reached 0.024%. SEM analysis revealed that cured WEP formed a dense cross-linked network with cement hydration products. This microstructural modification refined the pore structure, effectively addressing the material’s brittleness, ductility, and durability limitations.