View All Publications
1 December 2007 in Journal of Materials Science
Verified
Journal Article
Closed access
PDF file
SHS. Harosh
S. Harosh
LML. Miller
L. Miller
GLG. Levi
G. Levi
Menachem BambergerMenachem Bamberger
Menachem Bamberger

9 March 2006 in Journal of Materials Science
Verified
Journal Article
Closed access
PDF file
Menachem BambergerMenachem Bamberger
Menachem Bamberger

1 November 2011 in Journal of Materials Science
Verified
Journal Article
Closed access
PDF file
SAS. Avraham
S. Avraham
AKA. Katsman
A. Katsman
Menachem BambergerMenachem Bamberger
Menachem Bamberger

1 January 2020 in Heliyon
Verified
Journal Article
Open access
LALiraz Atia
Liraz Atia
Menachem BambergerMenachem Bamberger
Menachem Bamberger
The microstructure, tensile strength and impact strength following welding of Super-Duplex-Stainless-Steel using coated electrodes were investigated. It was observed that the lower the basicity index of the coating, the higher the reduction of oxygen in the weld pool. This can be explained by the interference of the basic elements with the oxygen reduction by the acidic elements of the coating. The change in the microstructure of the weld indicates the different cooling rate in each zone: The cooling rate during welding, from the highest to the lowest, is as follows: Interface area >>>Root area >>>Face area. In the face area, the highest content of austenite and lowest content of ferrite were observed, which indicates that this area has experienced the lowest cooling rate. In the interface area, the lowest content of austenite and the highest content of ferrite were observed, hence indicating that this area has experienced the highest cooling rate. All welds showed the presence of Widmanstӓtten austenite, grain boundary austenite, sigma phase and large grains of ferrite. It can be deduced that the sigma phase cannot be avoided in the welds; however, the secondary austenite can be avoided, by employing an appropriate "low heat input policy". It was found that the higher the content of the secondary austenite and sigma phases in the weld, the lower the yield stress, due to the brittle characteristics of these phases. However, the higher the austenite content in the weld, the higher the elongation.

11 October 2020 in SN Applied Sciences
Verified
Journal Article
Open access
PDF file
Alexander Katz-DemyanetzAlexander Katz-Demyanetz
Alexander Katz-Demyanetz
Menachem BambergerMenachem Bamberger
Menachem Bamberger
Michael RegevMichael Regev
Michael Regev
Mg65Cu25Y10 ribbons were produced by melt spinning. XRD, DSC, HRSEM and HRTEM were used to investigate their microstructure in its as-cast condition as well as after 3- and 6-minute exposures to 100 °C, 120 °C, 150 °C, 200 °C and 300 °C. XRD and DSC studies showed that the as-cast material had an amorphous character; the HRTEM investigation revealed that although the as-cast Mg65Cu25Y10 is known to be one of the best glass formers, it is nano-crystalline rather than amorphous. The fraction of the crystalline phase after each treatment was calculated by means of quantitative analysis that took into account the degree of crystallinity of the as-cast material as revealed by HRTEM. The current study showed that quantitative analysis may lead to serious errors when relying on the absence of crystalline peaks in the XRD spectrum as if the material is completely amorphous. Moreover, it seems that HRTEM examination is essential for carrying out quantitative XRD and DSC analyses. Graphic abstract

1 January 2006 in International Journal of Materials Research
Verified
Journal Article
Closed access
AFAmir Finkel
Amir Finkel
LSLudmila Shepeleva
Ludmila Shepeleva
Menachem BambergerMenachem Bamberger
Menachem Bamberger
EREugen Rabkin
Eugen Rabkin
The die cast Mg-5 wt.% Ca-6 wt.% Zn ternary alloy was exposed to 160 °C for different times of up to 40 days. Microstructural analysis and microhardness and hardness measurements of the samples after different exposure times enabled the thermal stability of the cast alloy to be monitored. The as-cast structure is composed mainly of α-Mg solid solution, elliptical grain boundary particles of CaMg2, and an intergranular eutectics of Mg and Ca2Mg6Zn3. The grain size of α-Mg and the structure of the alloy did not change during the treatment, but the amount of the intergranular phases increased slightly. Exposure to 160 °C resulted in a decrease in micro-hardness of the α-Mg grains, but no change in the overall hardness of the samples was observed. Microstructural analyses indicated diffusion of the solute elements from the α-Mg grains to the grain boundaries, resulting in a decrease in hardness of the α-Mg which is, however, compensated by an increase in hardness related to intergranular precipitates. Using a simple diffusion model, the diffusion coefficient of Ca atoms in Mg at 160 °C was estimated to be 2.1 · 10 –17 m2 s– 1, which is greater than that of Zn by two orders of magnitude.