Slime coating is known to have one of the detrimental effects of clay in coal flotation. In this study, the viscosity measurements of coal–clay-mixture suspensions and corresponding batch flotations were performed with increasing CaCl2 concentrations (ranged in 1–20 mM). It was found that at 4–6 mM concentration a significant transfer from Newtonian to non-Newtonian behavior occurred; meanwhile, the clay recovery increased dramatically. In this process, clay recovery through true flotation with entrainment excluded gradually increased. Cryo-SEM analysis, furthermore, confirmed that more coating clay appeared in higher CaCl2 concentrations. Thus, the rheology measurement could be used as a method for determining whether the slime coating occurred in flotation pulp with low salinity.
29 May 2024 in Environmental Science and Pollution Research