15 September 2019 in Materials
Verified
Journal Article
Open access
PDF file
YWYamin Wang
Yamin Wang
SHShaowei Hu
Shaowei Hu
ZHZhen He
Zhen He
In this paper, the mechanical and fracture properties of fly ash geopolymer concrete (FAGC) mixed with calcium aluminate cement (CAC) were explored. Fly ash was partially replaced by CAC with 2.5%, 5% and 7.5%. The results exhibit that the mechanical and fracture behaviors of FAGC are significantly influenced by CAC content. Based on the formation of more aluminum-rich gels, C-(A)-S-H and C-S-H gels, with the increase of CAC content, the compressive strength, splitting tensile strength and elastic modulus improved. Meanwhile, the peak load and effective fracture toughness show a monotone increasing trend. In addition, because C-S-H gels absorbed more energy, the fracture energy of FAGC increases. The maximal peak load, double-K fracture toughness and fracture energy reached up to1.79 kN, 4.27 MPam0.5, 10.1 MPam0.5 and 85.8 N/m with CAC content of 7.5%, respectively.

1 February 2019 in Construction and Building Materials
Verified
Journal Article
Closed access
YWYang Wang
Yang Wang
SHShaowei Hu
Shaowei Hu
XFXiangqian Fan
Xiangqian Fan
JLJun Lu
Jun Lu

18 March 2020 in Materials
Verified
Journal Article
Open access
PDF file
JWJuan Wang
Juan Wang
QWQianqian Wu
Qianqian Wu
JGJun-feng Guan
Jun-feng Guan
Peng ZhangPeng Zhang
Peng Zhang
HFHong-yuan Fang
Hong-yuan Fang
SHShaowei Hu
Shaowei Hu
The fracture performance of concrete is size-dependent within a certain size range. A four-phase composite material numerical model of mesofracture considering a mortar matrix, coarse aggregates, an interfacial transition zone (ITZ) at the meso level and the initial defects of concrete was established. The initial defects were assumed to be distributed randomly in the ITZ of concrete. The numerical model of concrete mesofracture was established to simulate the fracture process of wedge splitting (WS) concrete specimens with widths of 200–2000 mm and three-point bending (3-p-b) concrete specimens with heights of 200–800 mm. The fracture process of concrete was simulated, and the peak load (Pmax) of concrete was predicted using the numerical model. Based on the simulating results, the influence of specimen size of WS and 3-p-b tests on the fracture parameters was analyzed. It was demonstrated that when the specimen size was large enough, the fracture toughness (KIC) value obtained by the linear elastic fracture mechanics formula was independent of the specimen size. Meanwhile, the improved boundary effect model (BEM) was employed to study the tensile strength (ft) and fracture toughness of concrete using the mesofracture numerical model. A discrete value of β = 1.0–1.4 was a sufficient approximation to determine the ft and KIC values of concrete.


19 June 2020 in Frontiers in Materials
Verified
Journal Article
Open access
PDF file
LZLifei Zhang
Lifei Zhang
Yu ZhengYu Zheng
Yu Zheng
SHShaowei Hu
Shaowei Hu
JYJiasheng Yang
Jiasheng Yang
LXLipeng Xia
Lipeng Xia
The behavior of the bond between Engineering Cementitious Composites (ECC) and Glass Fiber Reinforced Polymer (GFRP) bar has a strong effect on the behavior of this composite structure. However, it is difficult to detect the failure mode and damage status of the interface using traditional testing methods. This is due to the strain-hardening mechanical behavior of ECC. An effective monitoring method using patch lead zirconate titanate (PZT) transducers and active sensing technology was used to detect the internal damage. In this active sensing technology, a PZT smart aggregate was bonded onto the middle surface of ECC, acting as a sensor. This study conducted a series of experimental studies on the bond behavior of GFRP-reinforced ECC based on pull-out tests. The test results are presented and discussed to investigate the bond-slip relationship and failure mechanism between FRP reinforcing bars and the ECC matrix. The status of interfacial damage between ECC and GFRP can be represented by the attenuation change of the stress wave. Finally, a damage index (DI) obtained using wavelet packet analysis is proposed to evaluate and quantify the level of FRP–ECC interaction damage. The analytical results reveal that the debonding and failure mechanism can be detected by using this DI index value, and the influence of the diameter of reinforcing bars should be considered, as should the Poisson's effect.

1 September 2019 in KSCE Journal of Civil Engineering
Verified
Journal Article
Open access
PDF file
YWYang Wang
Yang Wang
SHShaowei Hu
Shaowei Hu
JLJun Lu
Jun Lu
YQYanmin Qiao
Yanmin Qiao
This study examined the experiment of the water fracture interactions in the concrete. In order to create water pressure in the crack, a sealing device consisting of a mechanical clamp device and a waterproof membrane was proposed. Firstly, eighteen three-point bending tests were carried out to verify the proposed sealing device under three different loading rates. Subsequently, twelve hydraulic tests were performed under different loading rates. The results showed that the sealing device had minimal influence on the fracture behavior of concrete. Besides, with the increase of internal water pressure, the carrying capacity, fracture parameters and crack opening rate of concrete beam were evidently decreased. Meanwhile, the decrease of the carrying capacity, fracture parameters, and crack opening rate induced by internal water pressure decreased with the increase of loading rate. In addition, a significant hydraulic fracturing behavior caused by water pressure was observed in the quasi-static state.