Aging experiments are pivotal for car manufacturers to ensure the reliability of their battery cells. However, realistic aging methods are time-consuming and resource-intensive, necessitating accelerated aging techniques. While these techniques reduce testing time, they can also lead to distorted results due to the partially reversible nature of cell behavior, which stems from the inhomogenization and rehomogenization of conducting salt and lithium distribution in the electrode. To accurately capture these phenomena, cell relaxation must be incorporated into the test design. This work investigates the impact of the test procedure and several stress factors, namely depth of discharge and C- rate, on the formation and rehomogenization of cell inhomogeneities. The experimental results reveal increasing cell inhomogenization, leading to growing reversible capacity losses, particularly under conditions with shorter cycling interruptions (check ups and rest phases). These reversible capacity losses are associated with a significant reduction in cycle life performance of up to 400% under identical cycling conditions but shorter cycling interruptions. Similar trends are observed for increasing cycle depths and C-rates. Optimized recovery cycles effectively mitigate cell inhomogenization, doubling cycle stability without requiring considerable additional testing time. Furthermore, a clear correlation is found between increasing inhomogenization and cell failure, with lithium stripping confirming the occurrence of lithium plating shortly before failure. These findings emphasize the critical importance of considering cell relaxation in cycle aging studies to ensure reliable and accurate lifetime predictions. Under realistic conditions, substantially enhanced cycle stability is expected.
Spinel Li 4 Ti 5 O 12 (LTO): a promising “zero strain” anode for all-solid-state batteries (ASSB) offering exceptional cycling stability and prolonged battery lifespan.
Lithium-ion batteries are powering a revolution in electrification, but the underlying intercalation mechanism at the electrified interface remains poorly understood. Here, we provide experimental and theoretical evidence that lithium intercalation occurs by coupled ion-electron transfer (CIET), in which classical ion transfer from the electrolyte is coupled with quantum-mechanical electron transfer from the electrode to form an ion-electron pair in the reduced state. Current-voltage responses and reaction-limited capacities, corresponding to small and large overpotentials, respectively, were measured for common electrode materials and linked by the theory. The experiments showed universal dependence of the (de-)intercalation rate on Li-ion filling fraction, as well as temperature and electrolyte effects consistent with the theory. These results could be used to guide the design of high-rate battery interfaces that maximize the CIET reaction-limited current.