Welding thermal cycles with heat inputs ranging from 25 to 75 kJ/cm were performed on a Gleeble 3500. The impact energy improved significantly (from 10 to 112 J), whereas the simulated coarse-grain heat-affected zone (CGHAZ) microstructure changed from lath bainite ferrite (LBF) and granular bainite ferrite (GBF) + martensite/austenite (M/A) to acicular ferrite (AF) + polygonal ferrite (PF) + M/A as the heat input increased. Simultaneously, the mean coarse precipitate sizes and the degree of V(C,N) enrichment on the precipitate surface increased, which provided favorable conditions for intragranular ferrite nucleation. The Ar3 of CGHAZ increased from 593 °C to 793 °C with increasing heat inputs; the longer high-temperature residence time inhibited the bainite transformation and promoted the ferrite transformation. As a result, acicular ferrite increased and bainite decreased in the CGHAZ. The CGHAZ microstructure was refined for the acicular ferrite segmentation of the prior austenite, and the microstructure mean equivalent diameter (MED) in the CGHAZ decreased from 7.6 µm to 4.2 µm; the densities of grain boundaries higher than 15° increased from 20.3% to 45.5% and significantly increased the impact toughness. The correlation of heat input, microstructure, and impact toughness was investigated in detail. These results may provide new ideas for the development of high welding heat input multiphase steels.
For investigating the impact of ferritic morphology on yield strength (YS) of the high-heat-input welding induced coarse-grained heat-affected zone (CGHAZ) of a low carbon Mo-V-N-Ti-B steel, a group of particular welding heat inputs were designed to obtain different ferritic microstructures in CGHAZ. The tensile properties were estimated from typical samples with ferritic microstructures. The mixed microstructures dominated by the intragranular polygonal ferrite (IGPF), the intragranular acicular ferrite (IGAF), and the granular bainite (GB) were obtained at the heat inputs of 35, 65, 85 and 120 kJ/cm, respectively. When the main microstructure changed from IGPF to IGAF and GB, YS increased first and then decreased. The microstructure consisting mainly of IGAF possessed the maximum YS. As the main microstructure changed from IGPF to IGAF and GB, the contribution of grain refinement strengthening to YS was estimated to be elevated remarkably. This means the strength of CGHAZ in a low-carbon steel subjected to the high-heat-input welding could be enhanced by promoting the fine-grained AF and GB formation.
This study investigates the effects of molybdenum (Mo) and boron (B) on the microstructures and impact properties in the coarse grain heat-affected zone (CGHAZ) of a low-carbon V-Ti-N steel. The results demonstrate that, at a heat input of up to 75 kJ/cm, the addition of Mo alters the microstructure of the CGHAZ, transforming it from a polygonal ferrite (PF) + degraded pearlite (DP) composition to a granular bainite (GB) + a small amount of acicular ferrite (AF). This transformation increases the impact energy from 20 J to 35 J. Furthermore, with the Mo/B composite addition, the CGHAZ microstructure was refined due to the formation of a large number of acicular ferrites, and the mean equivalent diameter (MEDMTA≥15°) decreased from 7.9 μm to 4.2 μm. Consequently, the impact toughness of the CGHAZ increased from 35 J to 111 J. The correlation between the Mo/B elements, microstructure and impact toughness was investigated in detail. The findings of this study have the potential to generate novel ideas for the advancement of steel materials in the context of high heat input welding.
In this work, the influence of normalizing temperature on vanadium micro-alloyed P460NL1 steel is studied in terms of microstructures and impact toughness. With the normalizing temperature increased from 850 °C to 950 °C, the V(C,N) particles are dissolved. The dissolution of V(C,N) particles leads to a reduction in their ability to pin the primitive austenite grain boundaries, resulting in the coarsening of the primitive austenite grain. Simultaneously, the number of precipitated particles promoting ferrite nucleation decreased. The combination of these two effects led to the coarsening of ferrite grains in the steel samples. Of note, in the sample normalized at a temperature of 850 °C, the ferrite and pearlite crystals clearly exhibited banded structures. As the normalizing temperature increased, the ferrite–pearlite belt phase weakened. The highly distributed belt phase resulted in poor impact toughness of the steel sample normalized at 850 °C. The belt phase was improved at a normalizing temperature of 900 °C. In addition to that, the microstructure did not undergo significant coarsening at this normalizing temperature, thereby allowing it to achieve the highest toughness among all samples that were prepared for this study. The belt phase almost vanished at the normalizing temperature of 950 °C. However, microstructure coarsening occurred at this temperature, resulting in the deterioration of impact toughness.
In this work, the effect of nitrogen doping on vanadium micro-alloyed P460NL1 steel is studied in terms of microstructures and impact toughness. As the nitrogen content increased from 0.0036% to 0.0165%, the number of V (C,N) particles increased. The fine precipitates of V (C,N) effectively pin the prior austenite grain boundary, resulting in the refinement of the austenite grain. The intragranular and intergranular V-containing coarse particles enhanced the nucleation of intragranular ferrite and the grain boundaries of polygonal ferrite during air cooling. Accordingly, the proportion of heterogeneously nucleated ferrite increased, and the grain size of ferrite decreased. Notably, the size of the pearlite microstructure decreased, and the bainite microstructure appeared with a high doping of N. With the increase in N content, the impact toughness of vanadium micro-alloyed P460NL1 steel was enhanced. This can be attributed to the refinement of ferrite and the reduction in pearlite, which, in turn, was ascribed to the increase in nitrogen.