Electrodeposited composite coatings are widely studied for their potential to improve surface properties such as wear resistance and friction reduction. This study investigates the effect of electrodeposition parameters on the structure, morphology, and tribological performance of three coatings: pure nickel (Ni), Ni–graphite (Ni-G), and Ni–MoS2 (Ni-MoS2). Three deposition conditions were selected based on a review of key electrochemical parameters commonly used in the literature. The coatings were analyzed in terms of morphological characteristics, friction and wear resistance. The findings reveal that higher current densities led to increased friction and wear in Ni coatings, while lower pH values promoted finer crystallite sizes and improved tribological behavior. Ni-G coatings exhibited larger cluster formations with reduced friction and wear, especially at low pH, whereas Ni-MoS2 coatings developed a stable cauliflower-like morphology at pH 2, but showed reduced adhesion and structural integrity at higher pH levels. Scratch resistance tests performed under optimal deposition conditions showed that Ni-G coatings provided the highest resistance to mechanical damage, while Ni-MoS2 coatings were more susceptible to microcracking and adhesion failure. These results underscore the importance of optimizing deposition parameters to tailor the microstructure and functional properties of composite coatings for enhanced tribological and mechanical performance.
This research work focuses on the development and analysis of copper-filled linear low-density polyethylene (LLDPE) coatings deposited on LLDPE substrate via a thermocompression process. A dry mechanical mixing technique is employed to mix the copper–LLDPE powders. This relevant technology aims to develop new solid lubricating layered composite coatings without a negative environmental impact. Four different materials of the coatings are considered, i.e., LLDPE + 2 wt.% Cu, LLDPE + 6 wt.% Cu, LLDPE + 10 wt.% Cu and LLDPE + 20 wt.% Cu. The microstructural characterizations indicate a good degree of dispersion and adhesion between the continuous and dispersed phases at 20 wt.% Cu coatings. The mechanical properties of the pure polymer and the fully filled composite materials are investigated experimentally using tensile tests and Micro-Vickers hardness. The stiffness, hardness and mechanical strength of the composites are enhanced. Friction tests are also carried out via a linear reciprocating sliding tribometer. The incorporation of copper powder has a significant improvement on the friction and wear properties of the developed coatings. Higher copper powder loading provides a lower friction coefficient and wear volume loss. The best tribological performances are obtained with the LLDPE + 20 wt.% Cu coating. The wear mechanism of the LLDPE substrate is severe adhesive wear, and it becomes mild abrasive wear in case of the 20 wt.% Cu coating.
: An overview of the literature reveals that electrodeposition baths significantly influence deposited coatings’ morphology and properties. The present study investigates a sulphate-based bath in terms of the additive, pH, and temperature for the electrodeposition of Zn–Co alloys onto mild steel, achieving a nanocrystalline structure. The obtained results of the cyclic voltametric and SEM analyses revealed that sodium allowed the enhancement of cobalt electrocrystallisation (22.6 wt%) to homogenize further layers’ structure. However, the adjustment of pH allowed for the obtention of deposits with a refined structure containing only 5 wt% cobalt. Although an increase in room temperature resulted in deposit coatings with the same cobalt content, it notably produced a smoother structure. Subsequently, Zn–Co coatings were compared to pure zinc layers in terms of micromechanical and tribological behaviour. The morphology shifted from hexagonal platelets to nodular structures with the incorporation of cobalt, leading to an increase in microhardness. The morphology transformation, coupled with micromechanical reinforcement, contributed to the mitigation of friction and the improvement of the wear resistance of zinc layers through cobalt alloying. In fact, this improvement enhances the performance of zinc-coated applications in automotive and aerospace industries, particularly for standard assembly components that require adequate resistance to wear and abrasion during handling and tightening.