The flexural performance of RC beams strengthened with a novel high-strength and high-toughness epoxy mortar thin layer was investigated through four-point flexural tests on two contrast beams and two strengthened beams. The effects of this strengthening method on the failure modes, crack distribution, load–deflection curves, and bearing capacity of the RC beams with two reinforcement ratios were studied. The experimental results revealed that the contrast beams exhibited the typical bending failure modes where the failure mode of the reinforced beam is the yielding of the tensile reinforcement of the original beam and then fracture damage of the new epoxy mortar-reinforced thin layer. No debonding phenomenon was observed between the reinforced thin layer and the original concrete, and no visible cracks appeared before the tensile failure occurred in the thin layer. The cracks in the reinforced beams developed slowly, increased in number, and decreased significantly in width and spacing. The stiffness of the strengthened beam increased significantly, while its deformation ductility coefficient noticeably decreased. Compared to the corresponding contrast beams, the cracking load for strengthened beams A1 and B1 increased by 14% and 23%, respectively; the yield load increased by 32% and 40%, respectively; and the peak load increased by 18% and 17%, respectively. Finally, a calculation method for the flexural bearing capacity of RC beams strengthened with the novel epoxy mortar thin layer based on the flat section assumption was proposed. The calculated values showed a good agreement with the experimental values (with errors at −11.73% and 4.14%, respectively), providing a valuable reference for further research and application related to this kind of reinforcement method.
To investigate the axial compressive behavior of reinforced concrete-filled square glass-fiber-reinforced polymer(GFRP) tubular (RCFSGT) columns, 17 specimens were designed with variations in GFRP tube wall thickness, spiral reinforcement yield strength, and spiral reinforcement ratio. A detailed model was developed using the finite element software ABAQUS, enabling in-depth mechanistic analysis and expanded parameter studies. The results indicate that the failure types of the specimens are all manifested as GFRP square tube cracking, and the core concrete is subjected to crushing or shear failure. The inclusion of a reinforcement cage can significantly enhance the load-bearing capacity and ductility of the specimen. Furthermore, as the yield strength and reinforcement ratio of the spiral reinforcement increase, so does the load-bearing capacity of the specimen. The finite element simulation results align well with the experimental findings. As the wall thickness of the GFRP square tube increases from 2 mm to 6 mm, the load-bearing capacity improves by approximately 19.69%. With the yield strength of the spiral reinforcement rising from 200 MPa to 400 MPa, the specimen’s load-bearing capacity shows an increase of approximately 7.55%. However, as its yield strength continues to increase, there is minimal change in the load-bearing capacity. When the stirrup ratio of spiral reinforcement rises from 0.33% to 2.26%, the specimen’s load-bearing capacity experiences an increase of approximately 56.90%.
A total of five ultra-high-performance concrete (UHPC)-strengthened reinforced concrete (RC) columns and one RC column were built and subjected to eccentric compression testing to examine the force performance of UHPC-strengthened eccentrically compressed plain RC columns. This experimental study examined the crack progression, the damage morphology, the deformation ability, the maximum load-carrying capacity, and the ductile properties of the eccentrically compressed columns. It also investigated the impacts of eccentricity, the reinforcement thickness, and the addition of steel fibers on the effectiveness of reinforcement. The cracking load, peak load, and ductility coefficient of the UHPC-reinforced specimens were increased by 100.28%, 172.30%, and 56.30%, respectively, compared with the RC column at an initial eccentricity of 50 mm. As the eccentricity distance increased, the bearing capacity of the UHPC eccentrically compressed specimens decreased, and the deformation capacity increased. Increasing the steel fiber dosage within the appropriate range decreased the crack width of the specimen. The addition of 2% steel fiber resulted in a 24.8% increase in cracking load, an 8.96% increase in peak load, and a 2.60% increase in ductility coefficient compared to the addition of 1% steel fiber. However, the reinforcing effect of UHPC was weakened under high eccentric pressures. Based on the theory of concrete structure and mechanical principles, the formula for calculating the compressive bearing capacity of RC columns strengthened with high-performance concrete was proposed. The results of calculating the positive section bearing capacity of eccentrically compressed RC columns reinforced with high-performance concrete are in good agreement with the test values. The results of this paper provide an experimental basis and theoretical foundation for the cross-sectional design of UHPC eccentrically compressed columns.
This study aims to improve the shear performance of reinforced concrete (RC) beams by utilizing the favorable tensile and shear deformation capabilities of high-strength, high-toughness epoxy mortar. This study investigates the effect of reinforcement layer thickness on the shear failure modes, bearing capacity, and deformation capacity of beams through static tests on three specimens reinforced with thin layers of high-strength, high-toughness epoxy mortar and one unreinforced beam. The results show that reinforcing RC beams with thin layers of high-strength, high-toughness epoxy mortar can significantly enhance its shear bearing capacity and deformation capacity. The reinforcement layer of epoxy mortar can partially exert the shear resistance provided by the stirrups. The thicker the reinforcement layer, the more significant the improvement in the shear bearing capacity and deformation capacity of the strengthened beam. The epoxy mortar layer bonds well with the concrete, but delamination between the cover concrete and the core concrete leads to failure of the reinforcement layer, meaning that shear bearing capacity does not increase linearly with the thickness of the epoxy mortar layer. Based on the experimental results, a shear bearing capacity calculation formula for RC beams reinforced with thin layers of high-strength, high-toughness epoxy mortar is proposed, which matches the experimental results well.