A study has been conducted on the synthesis of HPG using Ultrasonic (USG) technology. The USG technology has been widely applied and successfully implemented in various chemical reactions and processes. However, little is known about the use of USG in the HPG synthesis process. The HPG process was conducted in room conditions for 150 minutes, with 4% NaOH as the catalyst, USG power of 200 watts and energy of 427,182 Joules. The process produced HPG with a molecular weight of 1,432 g/mol and a degree of polymerization (DP) of 7.518. FTIR analysis results showed the characteristic formation of the dendritic polyglycerol structure, indicated by the formation of ether or C-O-C groups at spectrum peaks between 1033 cm-1 and 1210 cm-1 and a spectrum peak at 3284 cm-1, indicating the presence of hydroxyl (O-H) groups. Identification using 13C NMR revealed peak shifts in the spectrum 71.5 to 72.8 ppm, identifying the HPG product as having a dendrimer structure. The 1H NMR spectrum showed peak shifts in the spectrum 3.2 to 3.6, identifying CH-O, indicating a dendritic structure.
A study was conducted on the synthesis of glycerol polymerization using ultrasonic (USG) technology. Although ultrasonication has been widely applied in various chemical processes, its role in glycerol polymerization remains insufficiently explored. In this study, polymerization was conducted under initial room-temperature conditions for 150 min using 4 wt% NaOH as a catalyst at an ultrasonic power of 300 W, corresponding to a cumulative energy input of 427,182 J. The process yielded a product with a molecular weight of 697.53 g/mol and a degree of polymerization (DP) of 7.52. FTIR analysis confirmed ether bond formation through characteristic C–O–C stretching bands in the 1033–1210 cm−1 region, while the broad O–H band at 3284 cm−1 indicated the presence of residual hydroxyl groups consistent with hyperbranched architectures. 1H-NMR spectroscopy further verified polymer formation, evidenced by the emergence of a doublet resonance at δ 3.68–3.69 ppm corresponding to ether linkages and the shift of the hydroxyl proton signal from δ 5.11 ppm in glycerol to δ 4.45–4.79 ppm in the polymer. Quantitative analysis using the Fréchet equation yielded a Degree of Branching (DB) of 0.57, characteristic of a well-defined hyperbranched architecture. This high DB ensures a dense periphery of hydroxyl groups, promoting excellent water solubility and versatile functionalization potential.