Three-dimensional concrete printing (3DCP) represents a paradigm shift in construction technology, enabling the automated, formwork-free fabrication of intricate geometries. Despite its rapid growth, successful implementation remains dependent on the precise control of material rheology and printing parameters. This review critically analyzes the foundational rheological properties of static yield stress, dynamic yield stress, plastic viscosity, and thixotropy and their influence on three core printability attributes, i.e., pumpability, extrudability, and buildability. Furthermore, it explores the role of critical process parameters, such as print speed, nozzle dimensions, layer deposition intervals, and standoff distance, in shaping interlayer bonding and structural integrity. Special emphasis is given to modeling frameworks by Suiker, Roussel, and Kruger, which provide robust tools for evaluating structural stability under plastic yield and elastic buckling conditions. The integration of these rheological and process-based insights offers a comprehensive roadmap for optimizing the performance, quality, and scalability of 3DCP.
Although 3D-printed concrete (3DPC) offers advantages such as faster construction, reduced labour costs, and minimized material waste, concerns remain about its long-term durability. This review examines these challenges by assessing how the unique layer-by-layer manufacturing process of 3DPC influences key material properties and overall durability. The formation of interfacial porosity and anisotropic microstructures can compromise structural integrity over time, increasing susceptibility to environmental degradation. Increased porosity at layer interfaces and the presence of shrinkage-induced cracking, including both plastic and autogenous shrinkage, contribute to reduced durability. Studies on freeze–thaw performance indicate that 3DPC can achieve durability comparable to cast concrete when proper mix designs and air-entraining agents are used. Chemical resistance, particularly under sulfuric acid exposure, remains a challenge, but improvements have been observed with the inclusion of supplementary cementitious materials such as silica fume. In addition, tests for chloride ingress and carbonation reveal that permeability and resistance are highly sensitive to printing parameters, material composition, and curing conditions. Carbonation resistance, in particular, appears to be lower in 3DPC than in traditional concrete. This review highlights the need for further research and emphasizes that optimizing mix designs and printing processes is critical to improving the long-term performance of 3D-printed concrete structures.
This review presents a comprehensive analysis of polypropylene (PP) fibre incorporation in three-dimensional printed concrete (3DPC), focusing on the material behaviour in both fresh and hardened states. PP fibres play a critical role in improving rheological properties such as buildability, flowability, and extrudability. While increased fibre content enhances interlayer bonding and shape retention through the fibre bridging mechanism, it also raises yield stress and viscosity, which may compromise extrudability. In the hardened state, PP fibres contribute to improvements in compressive and flexural strength up to an optimal dosage, beyond which performance may decline due to fibre clustering and reduced packing density. When aligned with the printing direction, fibres are particularly effective in mitigating shrinkage-induced cracking by redistributing internal tensile stress. However, their inclusion can lead to a slight increase in porosity and promote mechanical anisotropy. This review also discusses mix design parameters, fibre characteristics, and experimental protocols, while identifying key research gaps including the lack of standardized testing methods, limited understanding of fibre orientation effects, and insufficient exploration of hybrid fibre systems. Based on the synthesis of reported studies, optimal print quality and structural consistency have been associated with the use of 6 mm long fibres, nozzle diameters of 4 to 6 mm, and printing speeds ranging from 40 to 60 mm/s. Overall, PP fibre reinforcement shows strong potential for enhancing the structural integrity and dimensional stability of 3D-printed concrete, while emphasizing the need for further studies to optimize its use in practice.
Three-dimensional concrete printing (3DCP) is an emerging technology that improves design flexibility and material efficiency in construction. However, widespread adoption of 3DCP requires overcoming key material challenges. These include controlling rheology for pumpability and buildability and achieving sufficient mechanical strength. This paper provides a comprehensive review of the application of nanoclays (NCs) as a key admixture to address these challenges. The effects of three primary NCs (attapulgite (ATT), bentonite (BEN), and sepiolite (SEP)) on the fresh- and hardened-state properties of printable mortars are systematically analyzed. This review summarize findings on how NCs enhanced thixotropy, yield stress, and cohesion, which are critical for shape retention and the successful printing of multilayered structures. Quantitative analysis reveals that optimized dosages of NCs can increase compressive strength by up to 34% and flexural strength by up to 20%. For enhancing rheology and printability, a dosage of approximately 0.5% by binder weight is often suggested for ATT and SEP. In contrast, BEN can be used at higher replacement levels (up to 20%) to also function as a supplementary cementitious material (SCM), though this significantly impacts workability. This review consolidates the current knowledge to provide a clear framework for selecting appropriate NCs and dosages to develop high-performance, reliable, and sustainable materials for 3DCP applications.
Three-dimensional concrete printing (3DCP) is rapidly emerging as a transformative construction technology, enabling formwork-free fabrication, geometric flexibility, and reduced labour. However, the lack of conventional reinforcement and the strict requirements for fresh and hardened properties present significant challenges. Fibre reinforcement and supplementary cementitious materials (SCMs), such as ground granulated blast furnace slag (GGBS), offer pathways to enhance printability while mitigating environmental impact. This study investigates the combined effect of natural cellulose microfibres and silica fume on the rheological, mechanical, and sustainability performance of 3D-printable mortars. Six mixes were prepared with 50% GGBS, 45% cement, and 5% silica fume, incorporating fibre dosages from 0% to 1%. Results showed that a 0.5% fibre dosage provided the most favourable balance. At this dosage, static yield stress increased to 9.35 Pa and thixotropy reached 8623 mPa·s, enhancing structuration for shape retention. Plastic viscosity remained stable at 4–5 Pa·s, ensuring adequate extrusion performance. Higher fibre dosages (≥0.75%) caused a significant increase in rheological resistance, with static yield stress reaching 208 Pa and thixotropy 135,342 mPa·s. This resulted in excessive structuration, fibre clustering, and poor extrudability. Compressive strength was achieved at 109.10 MPa (92% of silica fume-only mix) with 0.5% fibre. In comparison, flexural strength was 13.20 MPa at 0.5% fibre content and reduced gradually to 12.29 MPa at 1% fibre due to weak fibre–matrix bonding and porosity. Sustainability analysis confirmed that using 50% GGBS and 5% silica fume reduced embodied carbon compared to a 100% cement mix. This study also demonstrated that cellulose microfibres at 0.25–0.5% are optimal for balancing fresh properties, mechanical strength, and sustainability in 3D-printed mortars.
This study investigates the durability challenges of 3D-printed concrete (3DPC) and examines the effect of silica fume (SF) on its performance, focusing on mechanical properties and selected durability tests as key indicators of mix suitability for 3D printing applications. Five low-carbon mixes were prepared with 50% GGBS replacement and varying silica fume contents (2.5–10%), and were evaluated through slump, compressive strength, rapid chloride migration, and accelerated carbonation tests. The addition of GGBS reduced the concrete’s shape retention, but incorporating silica fume improved flow behaviour, resulting in a more stable mix. The inclusion of GGBS and silica fume initially reduced 1-day strength but led to significant gains by 28 days, with the 5% SF low-carbon mix achieving the highest compressive strength. The low-carbon mixes showed superior chloride resistance, further enhanced by silica fume, though their carbonation resistance decreased with GGBS and SF addition. Overall, the 5% SF low-carbon mix demonstrated the best balance of strength, chloride resistance, and carbon reduction, despite minor trade-offs in early strength and carbonation resistance.