Since the machinability data on grade 3 austempered ductile iron is scarce, this experimental work mainly focuses on the impact of machining parameters on cutting force and surface roughness while turning the above work material with cubic boron nitride and tungsten carbide inserts. Parameters like depth of cut, cutting speed and feed were considered in this study when analyzing the machinability of austempered ductile iron. Austempered ductile iron was turned with CBN and coated WC inserts. The response surface methodology was utilized to design the experiments and optimize the cutting parameters for the work material by each of the above inserts. The cubic boron nitride insert performs well as compared to the coated tungsten carbide for turning the austempered ductile iron and it has been concluded by taking lower force and higher surface finish in to consideration. The optimum parameters for turning austempered ductile iron with the cubic boron nitride insert is as follows: 174 meter/minute cutting speed, 0.102 millimeter/revolution feed and depth of cut of 0.5 millimeter.
This work compares the effect of cubic boron nitride (CBN) and multilayer (TiCN+Al2O3+TiN) coated tungsten carbide (WC) tools during the turning of spheroidal graphite (SG) nodular iron. Nodular irons have more ductility which is required in mechanical components that demand high fatigue resistance like crankshafts, cam shafts, bearing caps and clutch housings. The impact of various process parameters like the depth of cut, cutting speed and feed on the surface roughness (Ra) of SG iron is studied and optimized using the response surface model. The chip morphology is also discussed for evaluation of the quality of the turned surface. The experimental outcomes reveal that the WC tool offers a high surface finish at the optimal combination of the cutting speed at 102 meter/minute, feed at 0.051 millimeter/revolution and depth of cut at 0.5 millimeter and that, for the CBN insert, at 245 meter/minute of cutting speed, 0.051 millimeter/revolution of feed and 0.75 millimeter of depth of cut.
Wing design is a very complicated and intricate issue. It is not feasible to cover everything in this chapter; however, it is possible to discuss some of the essential ideas that underpin design for high lift and low drag. Lift may be increased in four ways for fixed air characteristics and free-stream speed: increased wing area, increased angle of attack, increased camber, increased circulation through the use of high-momentum fluid. One of the most important applications of potential flow theory was the study of lifting surfaces such as aircraft wings, since the boundary conditions on a complex geometry can significantly complicate any attempt to tackle the problem via analytical techniques, which involves some simplification assumptions in order to arrive at a solution. These assumptions will be related to the concept of three-dimensional thin wing issues in this chapter.