Hydride phases based on the intermetallic compounds LaNi5, CeCo3, NdNi3, GdFe3, DyCo3, and ErNi3 have been synthesized at a hydrogen pressure of 10 MPa and a temperature of 273 K. The phase composition of the synthesized materials and the lattice parameters of the hydride phases have been determined by X-ray diffraction. During storage in air at room temperature, the hydrides decompose more slowly than do their analogs synthesized at low pressure. The hydrogen content of the hydrides is higher than or similar to that of hydride phases synthesized at high pressure. X-ray diffraction results for the low-temperature RT3-based intermetallic hydrides demonstrate that their lattice is expanded to a lesser extent than that of their high-pressure analogs.
A hydride phase containing 5.0 H atoms per formula unit has been synthesized in the CeNi3-H2 system at a hydrogen pressure of 5 MPa and a temperature of 273 K. The hydride is very stable during storage in air, with no hydrogen release. Its lattice parameters have been determined by X-ray diffraction for different synthesis conditions.
The magnetic properties of intermetallic compounds GdNi0.98Si0.02 and DyNi0.95Si0.05and hydrides based on them have been studied. It is found that a partial substitution of Si atoms for Ni...
The interaction of the V0.95Cu0.05, V0.94Co0.06, and V0.9W0.1 alloys with hydrogen has been studied at hydrogen pressures of up to 250 MPa. We have constructed hydrogen absorption/desorption isotherms at different temperatures and determined the thermodynamic parameters of the systems. According to X-ray diffraction data, the high-pressure hydride phases V0.94Co0.06H1.4 and V0.9W0.1H1.2 consist of a face-centered cubic phase similar in structure to the γ-phase of vanadium dihydride. In the case of the vanadium-copper alloy, the maximum composition of the hydride is V0.95Cu0.05H0.5.
CeNi3Hx (x = 0.7, 0.8, 1.0, 1.8, 3.4, 3.8) hydrides have been prepared through hydrogen desorption from CeNi3 hydrogenated at low (pH2 = 0.01 GPa) and high (pH2 = 0.2 GPa) hydrogen pressures. Using X-ray and neutron diffraction, the hydrides are shown to be isostructural with CeNi3 (sp. gr. P63/mmc, no. 194). The lattice parameters of the hydrides vary appreciably with hydrogen content. The sequence of hydrogen release from different interstices in the desorption process is shown to be opposite to that of hydrogen uptake in the hydrogenation process. The solid-solution range in the desorbed hydrides is much broader than that upon hydrogenation. The extent of the solid solution is influenced by the phase composition of the parent intermetallic compound.