Starch-based films are a valuable alternative to plastic materials that are based on fossil and petrochemical raw resources. In this study, corn and potato starch films with 50% glycerol as a plasticizer were developed, and the properties of films were confirmed by mechanical properties, surface free energy, surface roughness, and, finally, color and gloss analyses. Next, the films were overprinted using ink-jet printing with quick response (QR) codes, text, and pictograms. Finally, the print quality of the obtained prints was determined by optical density, color parameters, and the visual evaluation of prints. In general, corn films exhibit lower values of mechanical parameters (tensile strength, elongation at break, and Young Modulus) and water transition rate (11.1 mg·cm−2·h−1) than potato starch film (12.2 mg·cm−2·h−1), and water solubility is 18.7 ± 1.4 and 20.3 ± 1.2% for corn and potato film, respectively. The results obtained for print quality on starch-based films were very promising. The overprinted QR codes were quickly readable by a smartphone. The sharpness and the quality of the lettering are worse on potato film. At the same time, higher optical densities were measured on potato starch films. The results of this study show the strong potential of using starch films as a modern printing substrate.
Biodegradable films are a viable alternative to conventional plastics, thereby contributing to environmental pollution reduction. This study investigates the impact of substrate type on the properties of starch-based films produced using a plasticizer-assisted casting method. Four different substrates, namely, glass, copper, copper-free laminate, and Teflon®, were evaluated, addressing a research gap in which previous studies primarily focused on film composition. The films were analyzed for color, tensile strength, surface free energy, and surface morphology using optical and electron microscopy. The results demonstrated a substrate-dependent impact on surface properties, particularly optical transparency, surface roughness, and adhesion. The films cast on glass and laminate exhibited higher transparency and lower roughness, while copper substrate induced micro-striations and strong adhesion. Teflon® substrates replicated surface imperfections, which may be advantageous for optical applications, but caused film delamination. Tensile strength did not show statistically significant differences across substrates, although reduced elongation was observed for the films cast on Teflon®. Water vapor permeability was also not significantly affected, indicating a dominant role of bulk material properties. It averaged 25 kg per day per square meter, which means high vapor permeability. Surface free energy analysis revealed marked variations between top and bottom layers, with values ranging from 35 to 70 mJ·m⁻2 depending on the substrate. These findings confirm that the type of casting substrate plays a critical role in determining the surface and optical properties of starch-based films, even at the laboratory scale. This study provides new insights into substrate–film interactions and establishes a foundation for optimizing biodegradable film fabrication for industrial and application-specific needs.
This study investigates the properties of biopolymer films derived from semolina and farina, focusing on the effect of varying concentrations of glycerol as a plasticizer. The research fills a gap in the study of grains such as semolina and farina, which have the potential to expand the range of biodegradable materials. Mechanical tests revealed significant differences between the two film types. Farina-based films were notably more ductile, exhibiting an elongation at break of up to two times their original length, but with a low tensile strength of only 1–2 MPa. In contrast, semolina-based films were significantly stiffer, with a maximum elongation at break of 10%. A notable exception was the semolina film with a 25% glycerol concentration, which displayed an exceptionally high tensile strength of 17 MPa. This is a significant improvement over the typical potato starch-based film tested, which breaks at 5 MPa under static tearing. Furthermore, the study examined the films’ morphology, color, SFE, and surface roughness. Free surface energy ranged from 40 to 60 mJ/m2 in the tests, where the influence of the plasticizer was significant. Color tests clearly show yellow discoloration.