Background: Additively manufactured surgical guides require post-processing and subsequent decontamination prior to intraoral use. Steam sterilization and chemical disinfection protocols may influence the dimensional stability of polymer-based guide materials and potentially affect clinical fit and accuracy. Objectives: This in vitro study evaluated the dimensional changes of SLA 3D-printed Surgical Guide Resin V1 (Formlabs) after steam sterilization at 121 °C (AUT121) and 134 °C (AUT134) and after disinfection using 70% isopropyl alcohol (IPA70), compared with an untreated control group. Methods: Forty standardized specimens were fabricated using SLA technology and divided into four groups (n = 10/group): Control (CT), 121 °C steam sterilization (AUT121), 134 °C steam sterilization (AUT134), and IPA70 disinfection. Two linear measurement zones (L1 and L2) were assessed per specimen. Baseline measurements were recorded with a caliper (mm). Post-treatment measurements were obtained using microscopic evaluation, recorded in µm, and converted to mm for analysis. Dimensional change was calculated as ΔL = L_after − L_before. Within-group comparisons and between-group analyses were performed with a significance level of α = 0.05. Results: Steam sterilization at 134 °C (AUT 134) produced statistically significant dimensional changes in both zones (L1: p = 0.036; L2: p = 0.042). No statistically significant differences were observed in the AUT121 group (L1: p = 0.437; L2: p = 0.682) or the IPA70 group (L1: p = 0.164; L2: p = 0.086). Between-group analysis showed no significant differences for ΔL1 (p = 0.345), whereas ΔL2 differed significantly among groups (p = 0.021). Conclusions: Under the conditions of this study, AUT134 steam sterilization significantly affected the dimensional stability of SLA-printed Surgical Guide Resin V1 specimens. The AUT121 protocol and IPA70 disinfection did not result in statistically significant dimensional changes compared with baseline.
ECRIDA is a student project participating in the REXUS/BEXUS campaign that develops a UV resin 3D printer device capable of working in the low-gravity environment offered by the REXUS rocket flight. Our main objective is to describe the impact of low gravity on the UV resin 3D printing process by comparing samples printed on Earth with samples printed in space. Due to the requirements of the host vehicle and driven by the novel design of our device, a thorough testing campaign must be planned and completed to qualify the device for flight and maximise the success of the scientific objectives. This paper describes the requirements that the device must fulfil and goes into the design of our test plan describing the procedures and the results. Vacuum, vibration, pressure, and functional tests were performed and described together with our learned lessons and conclusions in our will to help student teams with their testing activities
Results of a study concerning the influence of impeller blade shape on increasing the efficiency of regenerative blowers are presented. Three impellers designed with different angles for the blades at inlet and outlet sections are considered: straight blades impeller (β 1 = β 2 = 90 0 ), forward twisted blades and backward twisted blades (β 1 = 90 0 ; β 2 = 105 0 ). Experimental research reported highest values for the pressure coefficients (Ψ) and flow coefficients (ϕ) for the impeller with forward twisted blades. In this case the values for the blower efficiency was 1.2-2% higher then those reported by the other two impellers and same casing. As the outlet blade angle is increasing and the blades are more twisted forward better performances are available. The solution of twisted blade is more effective then simply inclined blade when comparing the efficiency values at similar design data.