Separators are generally considered inert components in lithium-ion batteries. In the past, some electroactive polymers have been successfully applied in separator modifications for overcharge protection or as acid scavengers. This study highlights the first use of two “electroactive” carbazole polymers (copolymer 9-phenyl-9H-carbazole-phenyl [PCP] and poly(9-vinylcarbazole) [PVC]), which were each applied separately as coatings on the cathode-facing side of commercial Celgard 2325 separators, respectively, to enhance the cycling performance of 0.3Li2MnO3·0.7LiMn0.5Ni0.5O2//graphite (LMR-NM//Gr) full cells through interphase engineering. The team observed an irreversible polymer oxidation process of the carbazole-functionalized polymers—occurring only during the first charge—for the modified separator cells, and the results were confirmed by dQ/dV analysis, cyclic voltammetry measurements, and nuclear magnetic resonance characterizations. During this oxidation, carbazole polymers participate in the process of interphase formation, contributing to the improved cycling performance of LMR-NM//Gr batteries. Particularly, oxidation takes place at voltages of ~4.0 and ~3.5 V when PCP and PVC are used as separator coatings, which is highly irreversible. Further postmortem examinations suggest that the improvements using these modified separators arise from the formation of higher-quality and more inorganic SEI, as well as the beneficial CEI enriched in LixPOyFz. These interphases effectively inhibit the crosstalk effect by reducing TM dissolution.
23 February 2026 in Journal of the Electrochemical Society
In this work, a methodology utilizing potentiostatic holds is developed for measuring side-reaction rates at graphite (Gr) electrodes. The influence of Mn 2+ on parasitic reactions is evaluated in the presence of various preformed solid-electrolyte interphases (SEI). Gr SEI preformation was carried out using vinylene carbonate (VC) or lithium difluoro(oxalato)borate (LiDFOB) as an additive. In addition, a highly fluorinated electrolyte, free of traditional non-fluorinated organic carbonates, was used. Parasitic current increases were observed for all preformed Gr SEIs when Mn 2+ was present. Of the preforming electrolytes, the VC-derived SEI showed the lowest parasitic currents both with and without Mn 2+ .
15 October 2026 in Journal of the Electrochemical Society
Lithium-manganese-rich cathodes offer exceptional theoretical capacities but suffer from manganese dissolution/deposition, which limits performance. This work demonstrates that first-cycle electrochemical reduction can be modulated through electrolyte chemistry and applied C-rate. We show that solid-electrolyte interphase passivation quality is not an inherent guarantee of the reduction process, but rather a variable outcome of the specific electrochemical pathways triggered. While some reduction processes rapidly establish passivation, others consume substantially more electrolyte before the interface is effectively stabilized. Interphase engineering therefore requires careful, simultaneous selection of both the electrolyte formulation and applied C-rate.