Temperature and Cr content on the tensile and fracture mechanics properties of welded joints made of two Cr-Mo steels (A387 Gr. B and SA387 Gr. 91) are presented and analyzed. Tensile strength, yield stress and elongation, as well as the stress–strain curves are obtained by standard tensile tests using specimens extracted from welded joints. Fracture toughness testing was carried out to determine the critical stress intensity factor, KIc, and the critical crack length, ac, for all three zones of the welded joint, parent metal (PM), heat-affected zone (HAZ) and weld metal (WM). Based on these results, the tensile and fracture mechanics properties of welded joints made of A387 Gr. B and SA387 Gr. 91 steels are compared and analyzed.
Cracks are found during regular periodical NDT (MT and UT) in a large spherical tank, produced in 1974 of low carbon high quality steel of yield strength 385 MPa, similar to A516 Gr.60. Crack length was between 5 and 150 mm, with depth up to 13.8 mm, more than half of vessel thickness (26 mm). Repair was performed in the usual way, by grinding and surface welding. The waterproof testing of the repaired vessel was performed according to standard procedure with additional strain measurements using strain gauges positioned at surface welded regions to assess the vessel structural integrity. Also, acoustic emission was used to follow vessel behaviour during the waterproof test. Since no signal was recorded and strains were linear during the test, it was concluded that the repair was successful, and structural integrity is proved as well.