The recovery and recrystallization kinetics of 80% cold rolled ultra low carbon steel are investigated during isothermally annealing for temperature ranges 350–640 °C as a function of different annealing time. The recovery is assessed by magnetic coercivity (Hc), while the recrystallization is determined by mechanical hardness. At low temperature (350 to 520 °C) annealing, recovery dominates for long time (∼12 000 s), while the annealing at 550 °C/ 900s and 580 °C/ 300s causes the recrystallized nuclei formation . The recovery kinetics is introduced by differential rate equation, explaining the reduction in coercivity with the recovery progress and the variation of an activation energy from 41–113 kJ mol−1. The recrystallization kinetics is found faster at high annealing temperature 640 °C than 550 and 580 °C based on hardness measurement, justifying by apparent activation energy within 114–190 kJ mol−1. Furthermore, the recovery and recrystallization rate increase with different annealing time, consistent to the change of microstructures and grain boundary characteristics evaluated by the orientation imaging microscopy (OIM) of electron backscattered diffraction (EBSD).
The crystallization behaviour of Fe 70.8 Nb 3.7 Cu 1 Al 2.7 Mn 0.7 Si 13.5 B 7.6 alloy prepared in the form of amorphous ribbons by melt-spinning technique was studied using differential scanning calorimetry and the temperature variation in resistivity. An X-ray diffaction and transmission electron microscopy study showed the formation of f-Fe(Si, Al) and/or Fe 3 (Si, Al) nanoparticles after the first stage of crystallization. The activation energy for this nanophase formation was 68 kcal mol m1 . The brittleness of the alloy increased with the formation of nanoparticles after heat treatment. Superior soft magnetic properties were achieved when the material was heat treated at 790 K for 15 min. The particle size at the optimum heat treatment condition for superior soft magnetic properties was found to be 6.0 -0.5 nm which was less compared than for the Fe-Nb-Cu-Si-B system. The observed coercivity value at the optimum heat treatment condition was found to be 0.32 A m m1 (approximately 4 mOe). The presence of Al in the alloy reduced the particle size and the magnetic anisotropy energy of the system, which resulted in superior soft magnetic properties of the heat-treated materials.
The effect of annealing on melt spun Ni55Mn22Ga23 (at. %) ribbon has been addressed in terms of structural, thermal, thermomagnetic, and magnetic field induced strain (MFIS) behaviour. In comparison to as-spun ribbons, the samples annealed within the L21 domain at 1073 K for 30 h with subsequent furnace cooling, showed a rise in martensitic transformation temperature. This was endorsed from electron microscopy studies revealing change in morphology of martensite plate and stacking of dislocations in a preferential orientation. The mechanism is associated to martensitic accommodation which enhanced ferro-elastic magnetic coupling and also lowered magnetic coercivity. Such accommodations and adaptive anisotropy improved the MFIS behavior in the annealed sample.
11 April 2008 in Journal of Magnetism and Magnetic Materials
The paper addresses the structural, crystallization, soft magnetic and Curie temperature behaviour of Co36Fe36Si4B20Nb4 alloy. The material, prepared in the form of ribbons by melt-spinning technique, was amorphous in the as-cast state. Differential scanning calorimetry (DSC) showed two stages of crystallization whereas thermal variation of electrical resistivity (TER) carried out to a higher range of temperature indicated three stages of crystallization. The first crystallization stage, which occurred at 845 K and 825 K in DSC and TER, respectively, was due to the formation of nanophase (CoFe)2Si as evidenced by X-ray diffractometry (XRD) and transmission electron microscopy (TEM). The formation of these nanoparticles reduced the magnetocrystalline anisotropy, thereby revealing good soft magnetic properties in the samples annealed between 825 K and 875 K with coercivity less than 49.9 A m−1 (627 mOe) and susceptibility ∼ 0.72 × 103. In this optimum nanocrystalline state, the material also exhibited a high Curie temperature above 1100 K, opening the scope of the present nanocrystalline alloy for high temperature applications.