The electrocatalytic activity of electrodeposits of cobalt and Co-Mo alloys in the electroreduction reaction of hydrogen evolution in an acid, neutral and alkaline media has been studied in this work. To deposit coatings, a nontoxic citrate-pyrophosphate electrolyte was used, which was proposed earlier. It has been found that the alloys having the same chemical composition but a different phase composition can exhibit different electrocatalytic activity. The best electrolyte for the making of catalytically active Co-Mo alloys, for which the decrease in hydrogen evolution overpotential as compared with pure cobalt is about 400 mV at 30 mA cm−2 in alkaline solution, is solution with the cobalt and molybdenum concentration ratio 10:1.
1 March 2010 in Russian Journal of Applied Chemistry
Composition and the magnetic and corrosion properties of electrolytic Co-Mo alloys deposited from a polyligand citrate-pyrophosphate electrolyte were studied.
This paper compares the chemical composition, current efficiency, crystal structure, as well as the magnetic, electrocatalytic, and corrosion properties of CoRe electrolytic alloys.
The microstructure of silver coatings electrodeposited from different types of baths without brightening agents had been studied. The principal formulations of baths were following: cyanide: 0.75M KAg(CN)2+1.5M KCN+0.2M KOH; dicyanoargentate-thiocyanate (DCAT): 0.75M KAg(CN)2+6M KCNS + 1M K2CO3; dicyanoargentate-borate-phosphate-carbonate (BPC): 0.75M KAg(CN)2+0.82M KH2PO4+ 0.41M H3BO3+0.15M K2CO3+0.69M KOH; thiocyanate: 0.75M AgNO3 + 6M KCNS. The values of grain size was evaluated based on the XRD examination and are in the range 60 nm (for coatings electrodeposited from cyanide baths at current densities (15-40 mA cm-2) to 100 nm (for thiocyanate and BPC baths). The values of lattice parameter and interplanar distance obtained for Ag coatings are higher than that obtained for metallurgically prepared silver. Regardless on the type of bath, the obtained coatings were polycrystalline and nanocrystalline. The coatings electrodeposited at low current densities (< 10 mA cm-2) are rather crystalline that evidently was confirmed by SEM examination of surface morphology.