In this study, the performance of colemanite, which is a valuable boron waste, and recycled cathode ray tube glass (CRT) in the cement mortar was examined by experimentally. Colemanite waste (CW) and CRT were replaced with cement and aggregate and used as mineral additives, and their effect on the physical and mechanical properties (PP and MP) of mortar was investigated. In addition to the reference sample that didn’t contain CW or CRT, seven more samples were used. In these samples, cement was used at a rate of 2.5% along with CW, and the aggregate was replaced with CRT at the rates of 10%, 20%, and 30%, and with the combination of CW and CRT. The workability, unit weight, and water absorption, compressive strength (CS), flexural strength (FS), and abrasion resistance properties of the mortars were compared. As a result of this study, it has been observed that the use of waste materials can make positive contributions to some of the PP and MP of the mortar. Thus, the goal of both improving the properties of the mortar and making it affordable by using waste materials were achieved.
4 November 2026 in Journal of Materials in Civil Engineering
This study investigates the durability performance of waste rubber fiber (RF)-reinforced geopolymer concrete (RGPC) by evaluating the effects of rubber fiber content, ground granulated blast furnace slag (GGBS) percentage, and curing temperature (CT) using an Taguchi design. The influence of RF (0.6%, 0.9%, 1.2%), GGBS [25% GGBS–75% fly ash (FA), 50% GGBS–50% FA, and 75% GGBS–25% FA], and CT (75°C, 90°C, 105°C) on water absorption (WA), sorptivity, water permeability, magnesium sulfate ( ) resistance, and drying shrinkage was examined. Microstructural characteristics were assessed through scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDX) analyses, and the statistical significance of each parameter was determined using ANOVA. Increasing the GGBS percentage markedly improved transport-related durability: water absorption decreased from 5.62% at 25% GGBS to 2.31% at 75% GGBS (a 58.9% reduction), and the initial sorptivity coefficient decreased fourfold. Water penetration depth also decreased from 50 to 22.7 mm with higher GGBS content. RF incorporation increased water absorption and sorptivity but enhanced resistance; mixes with high FA content exhibited ultrasonic velocity increases of up to 9.86% after 12 weeks of exposure. Increasing the CT from 75°C to 105°C reduced drying shrinkage from 0.052% to 0.023%, representing nearly a 50% improvement. SEM–EDX results confirmed that higher GGBS levels produced denser C─(N)─A─S─H gel structures, consistent with improved durability. Overall performance optimization identified the A1B3C3 mix (0.6% RF, 75% GGBS, 105°C CT) as the optimum combination. Among all parameters, GGBS proved to be the dominant factor influencing RGPC durability.