8 August 2019 in Metals
Verified
Journal Article
Open access
PDF file
JSJinlong Su
Jinlong Su
XQXiaoming Qiu
Xiaoming Qiu
FXfei xing
fei xing
YRYe Ruan
Ye Ruan
Laser-welded forged steel pistons can meet the needs of the new era of heavy truck engines. 42CrMo4 and 38MnVS6 are widely used as piston materials due to the good mechanical properties. This study investigates the influence of preheating on microstructure and mechanical properties of 42CrMo4/38MnVS6 laser welding joint. The experimental results show preheating increases the laser absorption capacity of the metal, which can lead to an increase in weld width. The microstructure of weld is the high-hardness and poor toughness twin martensite without preheating. As the temperature of preheating increases, the twin martensite in the weld begins to transform into lath martensite and regenerates ferrite and bainite. As the preheating temperature increases, the plane fracture toughness (K1C) of the weld increases and then decreases, reaching the highest value of 2322.94 MPa·mm−1/2 at 150 °C. Compared with no preheating conditions, the tensile strength of the welded joint after preheating is improved. The fracture mode of welded joints changes from brittle fracture to ductile fracture. When the preheating temperature is 100–200 °C, the tensile strength of the welded joint reaches 1018.1–1032.5 MPa; when the preheating temperature is 250 °C–300 °C, the tensile strength decreases.

1 May 2016 in Journal of Alloys and Compounds
Verified
Journal Article
Closed access
FXFei Xing
Fei Xing
QSQinghui Shang
Qinghui Shang
YLYuzhen Lu
Yuzhen Lu
JLJingwei Liang
Jingwei Liang
XQXiaoming Qiu
Xiaoming Qiu

24 February 2015 in Journal of Materials Engineering and Performance
Verified
Journal Article
Closed access
PDF file
FXFei Xing
Fei Xing
XQXiaoming Qiu
Xiaoming Qiu

9 July 2018 in Metals
Verified
Journal Article
Open access
PDF file
JDJiawei Ding
Jiawei Ding
XQXiaoming Qiu
Xiaoming Qiu
GDGang Ding
Gang Ding
YRYe Ruan
Ye Ruan
In this paper, a wear-resistant alloy with the chemical composition of 16 wt% Cr-3 wt% B-0.6 wt% C-1 wt% Mn-Fe, in which M2B was the antifriction skeleton, was prepared in a medium-frequency induction furnace. The microstructure and mechanical properties were experimentally investigated. The results show that the microstructure of the Fe-Cr-B alloy was composed of lath martensite and clavate, reticular, and clustering borides (M2B). After the thermal treatment, the morphology, chemical composition, and volume fraction of the M2B did not change significantly. Because of the reduction in element saturation, secondary borides M23(B,C)6 precipitated from the matrix, which resulted in a decrease in matrix microhardness. As a result, the bulk hardness and abrasive resistance of the alloy accordingly decreased, and the impact toughness inversely increased. According to the results of XRD, electronic probe microanalyzer (EPMA), and TEM, the chemical formula of M2B was FeCr0.89Mn0.14(B,C), which resulted in a body-centered tetragonal (BCT) structure. The chemical formula of the M23(B,C)6 was Fe17.97Cr4.13Mn1.14 (B,C)6, which resulted in a face-centered cubic (FCC) structure.